Henkel
Adhesives, Electronics Assembly, and Thermal Management Solutions
Henkel supplies industrial adhesives, sealants, electronics assembly materials, encapsulants, die attach technologies, thermal interface materials, and specialty process chemistries for applications across automotive, aerospace, electronics, semiconductor, industrial manufacturing, and other markets. Its industrial portfolio includes product families and brands such as Loctite, Bonderite, Frekote, Stycast, Eccobond, and Bergquist, with chemistry, cure method, packaging, and processing requirements varying by product and application.
As an authorized Henkel distributor, Krayden supplies a selection of Henkel industrial and electronic materials and provides technical guidance for material selection, product comparison, substrate and application requirements, dispensing, and process considerations.
Markets Served by Henkel
Featured Henkel Brands
Six Henkel brands covering industrial bonding, surface treatment, mold release, electronics protection, and thermal management materials.

Loctite™
Adhesives, sealants, and surface-treatment chemistries spanning structural bonding, gasketing, instant adhesives, epoxies, silicones, and electronics assembly applications.

Bonderite™
Metal pretreatment and surface technologies including industrial cleaners, conversion coatings, and related preparation chemistries for aluminum, steel, and other substrates.

Frekote™
Mold release agents, sealers, and cleaners used to support composite, rubber, and other molding operations where controlled release and mold maintenance are required.

Stycast™
Epoxy and silicone potting and encapsulation materials used to protect sensitive circuitry and electronic assemblies from mechanical and environmental exposure.

Eccobond™
Electronics protection and assembly materials including underfills, liquid encapsulants, optically clear materials, and other formulations used around semiconductor and electronic packages.

Bergquist™
Thermal interface materials for transferring heat between electronic components and heat sinks or enclosures, including gap pads, dispensable gap fillers, and thermal compounds.
Adhesives & Sealants
Henkel adhesives and sealants span general-purpose and structural bonding materials alongside gasketing sealants for industrial assembly and sealing. The source portfolio includes epoxy, silicone, acrylic, anaerobic, and other product-specific chemistries. Selection depends on the substrates, cure process, required handling time, environmental exposure, joint or flange geometry, and service conditions.
Encapsulants & Underfills
Henkel encapsulation and underfill materials protect electronic components, interconnects, and assemblies from mechanical and environmental stresses. The source portfolio includes potting systems, liquid encapsulants, low-pressure molding materials, capillary underfills, and optically clear formulations. Selection depends on package geometry, material flow, cure method, thermal-mechanical requirements, environmental exposure, and production process.
Electronics Assembly Adhesives & Inks
Henkel electronics assembly materials include film and paste adhesive technologies used for component attachment, structural bonding, electrical interconnection, grounding, and EMI-management functions. Depending on the application, materials may be electrically conductive or insulating and may be supplied in film, paste, coating, or other product-specific formats. Selection should account for the assembly geometry, electrical function, deposition method, cure process, and production requirements.
Die Attach
Henkel die attach materials support bonding of semiconductor die to substrates, leadframes, and package structures using film, paste, sintering, and coating-based approaches. Required electrical conductivity, thermal transport, bond-line control, metallization, cure or sintering conditions, and production method vary by material and package design.
Thermal Interface Materials
Henkel thermal interface materials support heat transfer between electronic components and heat sinks, cooling plates, or enclosures. The source portfolio includes Bergquist gap pads, dispensable one-part and two-part thermal materials, and thermal greases. Selection depends on thermal conductivity, gap thickness, compressibility or bond-line control, dielectric requirements, dispensing method, and assembly process.
Specialty Chemicals, Molding Compounds & Mold Maintenance
Henkel specialty and mold-support materials include cure components, low-pressure molding compounds, mold-cleaning materials, mold-release agents, and surface-preparation chemistries. Henkel currently offers low-pressure molding materials under TECHNOMELT and LOCTITE for electronic overmolding, while process and maintenance materials support compatible resin systems, molds, and downstream bonding or coating operations.
Talk to our Henkel Experts
Krayden can help compare Henkel materials for bonding, sealing, encapsulation, underfill, electronics assembly, die attach, and thermal management applications. Our team can support product selection, substrate and application requirements, process considerations, and comparison of candidate materials for your assembly.
Henkel Quick Reference
1039 products
-
LOCTITE ABLESTIK 8008
- Snap curable after B stage
- Low modulus
- Void free bondline without bleed
-
-
LOCTITE ABLESTIK ABP 8068TA
- Excellent workability
- Dispensable
- Printable
-
LOCTITE ABLESTIK SSP 2020
- High thermal conductivity
- High electrical conductivity
- High die shear strength
-
-
-
LOCTITE ABLESTIK 16-1LV
- Two components
- Room temperature cure
- Low volume resistivity
-
-
-
-
-
-
-
-
-
-
-
-
-
-
LOCTITE ECI 8001 E&C
- Rapid heating with fast, defined cut-off temperatures, no external control devices needed
- Printable on most common substrates
- Screen printable
-
-
LOCTITE ABLESTIK 8700E
- Electrically conductive
- Retains high shear strength after thermal cycling
- Thermally conductive
-
LOCTITE ABLESTIK ABP 8068TD
- Good workability
- ±50 W/mK Thermal Conductivity
- High electrical conductivity
-
LOCTITE ECCOBOND D125 F DR
- Low water absorption
- Low exotherm
- Non-sag
-
-
-
-
-
-
LOCTITE ABLESTIK 2025DNP
- Excellent dispense capabilities
- For mother die in array packaging
- 260ºC reflow capability for Pb-free applications
-
LOCTITE ECI 1014 E&C
- Low temperature drying
- High conductivity
- Compatible for use with polycarbonate, polyester and polyurethane
-
LOCTITE ABLESTIK FS 849-TI
- Low outgassing
- Low electrical resistance
- High thermal conductivity - 7.8 W/mK
-
-
-
LOCTITE ABLESTIK ABP 6395T
- High reliability
- 30 W/(m-K) Thermal Conductivity
- Good adhesion to Ag, Cu, PPF, Non-BSM, and BSM die
-
LOCTITE ABLESTIK ATB 125GR
- Low ionic content
- Excellent adhesion on both metal lead frames and BGAs
- High modulus
-
-
LOCTITE ABLESTIK ABP 6392TEA
- High electrical conductivity
- High thermal conductivity
- Good adhesion to a variety of substrates
-
LOCTITE ABLESTIK ABP 8068TI
- High thermal and electrical properties
- Low sintering temperature
- High reliability
-
-
LOCTITE ABLESTIK NCA 2390
- High dispense aspect ratio
- Fast cure at low temperature
- High thixotropic index
-
-
-
LOCTITE ABLESTIK 958-7 | Electrically Conductive Adhesive
- Electrically conductive
- Good adhesion to gold
- Heat cure
-
LOCTITE 3296 | UV-curable Epoxy Adhesive
- Fast UV cure
- High Tg and low CTE
- Low shrinkage during & after cure
-
LOCTITE ABP 2100ANP | PFAS-Free Die Attach Adhesive
- Formulated for Pb-free applications
- High hot/wet adhesion
- Excellent dispensability
-
LOCTITE 3626M | Surface Mount Adhesive
- Heat-cured
- For SMD components to PCB
- Compatible with syringe and stencil print
-
-
-
Loctite 495
- One-Part Adhesive Form
- Multi-Substrate Assembly Fixturing
- Low-Viscosity Adhesive Application
-
Loctite 580 Pipe Sealant
- One-Component Sealing System
- Low Pressure Sealing for Inactive Metals
- Room-Temperature Sealing Cure
-
Loctite Ablestik 83C Conductive Epoxy Adhesive
- Silver-Filled Epoxy Adhesive
- 0.0004 ohm-cm Volume Resistivity
- Electrical-Connection Epoxy Bonding
-
Loctite Ablestik 2116 Non-Conductive Adhesive
- Metal/Glass/Ceramic/Plastic Staking and Bonding
- 30-Minute Pot Life
- 415 V/mil Dielectric Strength
-
-
BONDERITE C-AK ALUM ETCH 2 AERO
- Cleaning and Etching
- Uniform Surface Wetting
- Aluminum Surface Treatment
-
BONDERITE C-AK ALUM ETCH 3 AERO
- Surface Soil Removal
- Aluminum Surface Etching
- 0.05 to 0.10 mil/min Etch Rate
-
BONDERITE C-IC DEOXIDOZER
- Aluminum Deoxidizing, Desmutting, Etching
- Prepares for Chromating
- 1 to 10 Minute Application Rate
-
Loctite Ablestik CT 5047-2
- Electrically Conductive Bonding
- Room Temperature Curing
- Electrical Connections Bonding
-
BONDRITE C-AK MIL-ETCH
- Fine Satin or Frosted Etch on Aluminum
- Low-Foam Alkaline Formulation
- Scale- and Sludge-Reducing Sequestering Chemistry
-
FREKOTE 44NC
- Multi-Cycle Mold Release
- Reduced Mold-Surface Contamination Risk
- Non-Silicone Downstream-Compatible Formulation
-
FREKOTE RC-321
- Consistent Multi-Cycle Mold Release
- Reduced Resin Adhesion to Mold Surfaces
- Semi-Permanent Low-Residue Coating
-
Loctite FREKOTE R-110
- Multi-Cycle Mold Release
- Reduced Resin Adhesion to Molds
- Semi-Permanent Low-Residue Coating
-
-
-
-
LOCTITE ABLESTIK 2101
- 23 N/mm^2 Aluminum Lap Shear
- High-Resistivity Electrical Insulation
- Fuel, Oil, and Acid Resistance
-
LOCTITE ABLESTIK 2106T
- Shore D 72 within 60 Minutes
- 410 V/mil Dielectric Strength
- Metal-to-Masonry Multi-Substrate Bonding
-
LOCTITE ABLESTIK 2112
- Critical Electronics/Aerospace Bonding
- Non-Sag PCB Component Staking
- Electrical Insulation and Environmental Resistance
-
LOCTITE ABLESTIK 2113
- Low-Viscosity Optical Bonding
- Fine-Detail Flow and Wetting
- Electrically Insulating Cured Adhesive
-
LOCTITE ABLESTIK 2114
- Optically Clear Bonding
- 50 N/mm^2 Cured Tensile Strength
- Broad Metal/Glass/Ceramic/Plastic Compatibility
-
ABLESTIK 2115
- Shock- and Temperature-Cycling Resistance
- Low-Viscosity Precision Optic Bonding
- 60-Watt Laser-Energy Resistance
-
ABLESTIK 2135D
- Tough, Durable Epoxy for Bonding, Laminating, Sealing
- 1,200 mPa s Mixed Viscosity
- 2.7 x 10^13 ohm-cm Volume Resistivity
-
ABLESTIK 2143D
- Medium-Viscosity Application Control
- 1 x 10^14 ohm-cm Volume Resistivity
- Room-Temperature Adhesive Cure
-
ABLESTIK 2156
- 0.84 W/(m K) Thermal Conductivity
- Heat-Sensitive Component Staking
- -70 to 100 deg C Operating Range
-
ABLESTIK 2158
- Electrically Insulating Staking Epoxy
- Flexible Mismatched-Adherend Bonding
- 2 x 10^15 ohm-cm Volume Resistivity
-
-
ABLESTIK 2332-17U
- Solvent-Free Bonding Formulation
- 90-Minute 100 deg C Cure
- 24 N/mm^2 Aluminum Lap Shear
-
-
ABLESTIK 286
- 1.04 W/(m K) Thermal Interface
- 30-Minute Working Window
- Room-Temperature Thermal Interface Cure
-
ABLESTIK 2907
- Electrically Conductive Bonding
- Room-Temperature Adhesive Cure
- Glass-to-Plastic Epoxy Bonding
-
ABLESTIK 293-1
- Difficult-Substrate General Assembly Bonding
- 37.9 N/mm^2 Aluminum Lap Shear
- 3.20 x 10^14 ohm-cm Volume Resistivity
-
ABLESTIK 293-21
- Strong Bonding to Difficult Metallic Substrates
- 90-Minute 75 deg C Cure
- 1.0 x 10^13 ohm-cm Volume Resistivity
-
-
-
-
ABLESTIK 550
- Film-Format Bonding for Difficult Surfaces
- 30-Minute 150 deg C Cure
- 39 N/mm^2 Aluminum Lap Shear
-
ABLESTIK 568
- 2.5 x 10^14 ohm-cm Volume Resistivity
- 2-Hour 95 deg C Cure
- 3 mil Glass-Fabric-Supported Film
-
-
-
ABLESTIK 77-1S
- One-Component, Solvent-Free Epoxy for Attaching Surface-Mounted Devices
- Smooth Non-Tailing Non-Sag Consistency
- 91-Day Working Window
-
ABLESTIK 77-2LTC
- One-Component, Solvent-Free Epoxy for Attaching Surface-Mount Devices
- Smooth Non-Tailing Non-Sag Consistency
- 2.5 x 10^14 ohm-cm Volume Resistivity
-
ABLESTIK 816H01
- 2.0 W/(m K) Thermal Interface
- Three-Hour Working Window
- Room-Temperature Thermal Interface Cure
-
ABLESTIK 8380
- Reduced Tailing and Stringing in Smart-Card Assembly
- 1-Minute 150 deg C Cure
- 0.0005 ohm-cm Volume Resistivity
-
ABLESTIK 83CJ
- 0.0004 ohm-cm Volume Resistivity
- 45-Minute Working Window
- Cold-Solder-Type Electrical Connections
-
ABLESTIK 84-1LMINB
- 0.0001 ohm-cm Volume Resistivity
- Screen-Printable Epoxy Bonding
- 30-Minute Working Window
-
ABLESTIK 85-1
- Gold-Filled Conductive Die-Attach Adhesive
- 49 N/mm^2 Shear Strength
- 1-Hour 150 deg C Cure
-
-
ABLESTIK 976-1
- Electrically Conductive Thermal Interface
- 2.1 W/(m K) Thermal Interface
- 1:1 Meter-Mix Processing
-
ABLESTIK CF3366
- 0.0003 ohm-cm Volume Resistivity
- 5.17 N/mm^2 Aluminum Lap Shear
- Flexible Cured Adhesive
-
ABLESTIK CT5047-2
- Conductive Bonding for Temperature-Sensitive Electrical Connections
- 24-Hour 25 deg C Cure
- 2-Hour Working Window
-
ABLESTIK ECF 550
- Conductive Grounding and RF-Shielding Film
- Controlled Film Processing with Flexible Supply Formats
- 20 N/mm^2 Lap Shear
-
ABLESTIK ECF 561E
- Electrically Conductive Bonding
- Flexible Cured Adhesive
- 1.6 W/(m K) Thermal Conductivity
-
ABLESTIK ECF 568
- Electrically Conductive Application
- 2-Hour 95 deg C Cure
- Sheet Stock or Die-Cut Preforms
-
ABLESTIK G 909
- High-Strength Structural Bonding
- Thixotropic Non-Sag Placement
- 90-Minute 100 deg C Cure
-
ABLESTIK KE 4238
- Conductive Bonding for Heat-Sensitive Assemblies
- 21 W/(m K) Thermal Conductivity
- 2-Hour 60 deg C Cure
-
ABLESTIK KS 0004
- 0.01 ohm-cm Volume Resistivity
- 2-Hour 60 deg C Cure
- Conductive Bonding and Encapsulation Utility
-
ABLESTIK KS 4008
- 0.01 ohm-cm Conductive Bonding
- Aircraft Static-Discharger Bonding
- Room-Temperature or Heat Cure
-
-
BONDERITE C-AK 298
- Non-Silicated Aluminum Immersion Cleaner
- Multi-Soil Removal and Free Rinsing
- 54 to 82 deg C Immersion Cleaning
-
BONDERITE C-AK 4215 NC-LT
- Low-Temperature Multi-Metal Cleaning
- Fuel/Hydraulic Component Cleaning
- Chromate-Free Low-Foam Noncorrosive Formulation
-
BONDERITE C-AK 4316
- Heat-Scale Conditioning for Multiple Alloys
- Lower-Temperature Molten-Salt Bath Processing
- Nonflammable Titration-Controlled Bath Maintenance
-
BONDERITE C-AK 4338LP1
- Two-Part Alkaline-Permanganate System Component
- Jet-Engine Heat-Scale Conditioning
- Liquid-Concentrate Bath Make-Up
-
BONDERITE C-AK 4338LP2
- High-Temperature Oxide-Scale Conditioning
- Equal-Volume Two-Liquid Mixing
- 15 to 25% Component Concentration
-
BONDERITE C-AK 5948-DPM
- Painted/Unpainted Aircraft Cleaning
- Nonstaining Free-Rinsing Aluminum Cleaning
- Phosphate/Chromate-Free Immersion/Ultrasonic Cleaning
-
-
BONDERITE C-AK 909
- Heavy-Soil Multi-Metal Degreasing
- Immersion or Ultrasonic Cleaning
- Caustic-Soda-Free Chelating Formulation
-
BONDERITE C-AK ALTREX
- Inhibited Non-Etching Aluminum Cleaning
- BAC-5749 Medium-Duty Soak Qualification
- Buffered Hard-Water Bath Control
-
BONDERITE C-AK ALUM
- Removal of Light Soils with Immersion Etching
- Promotes Uniform Wetting Through Low Surface Tension
- 40 to 80 deg C Service Range
-
BONDERITE C-AK EC
- Multi-Soil Phosphate-Line Equipment Cleaning
- Spray, Immersion, or Recirculation Cleaning
- Two-Step Descaling Bath Control
-
BONDERITE C-AK ETCH 9HL
- High-Copper Aluminum Chem-Mill Processing
- Controlled Immersion Chemical Milling
- Improved Line Definition and Etch Uniformity
-
BONDERITE C-AK LS
- Rolling-Oil Steel-Strip Cleaning
- Dip, Spray, or Electrolytic Cleaning
- Oil-Separating Emulsion Behavior
-
BONDERITE C-AK MIL-ETCH
- Uniform Fine Satin or Frosted Etch
- Low-Foam Low-Mist Alkaline Etching
- BAC 5786 Operating Conditions
-
BONDERITE C-AK VITKL
- Ferrous/Titanium Tenacious-Soil Removal
- Boeing BAC 5749 Compliance
- Low-Foaming Quick-Rinse Bath Control
-
BONDERITE C-IC 2310
- Chromium-Free Aluminum Deoxidizing Cleaner
- No-Heat Immersion/Spray Cleaning
- MIL-W-6858C Deoxidizing Compliance
-
BONDERITE C-IC 33
- Non-Flammable Bonding Formulation
- Brush, Spray, or Immersion Application
- Adhesion-Promoting Surface Treatment
-
BONDERITE C-IC 4409
- Ferrous/Nonferrous Alloy Cleaning and Deoxidizing
- Hand-Wipe, Immersion, or Spray Processing
- Water/Steam-Rinsable Rust Removal
-
BONDERITE C-IC 457
- Heavy-Oxidation Aluminum/Magnesium Deoxidizing
- Non-Flammable Phosphate-Free Formulation
- Pre-Paint Surface Conditioning
-
BONDERITE C-IC 79
- Phosphoric-Acid Oxidation/Corrosion Cleaner
- Brush, Immersion, or Spray Application
- Pre-Paint/Conversion-Coating Surface Preparation
-
BONDERITE C-IC ALDOX
- Chromate-Free Aluminum Deoxidizing and Desmutting
- Boeing BAC 5765 Qualification
- Ambient Spray or Immersion Processing
-
BONDERITE C-IC SMUTGO
- Chromate-Free Acid Cleaner
- Ambient Immersion or Spray Processing
- Low Electrical Surface Resistance
-
BONDERITE C-SO 2382
- Aerospace NESHAP/AQMD Solvent Compliance
- Fast-Evaporating Residue-Free Surface Prep
- Noncorrosive Ferrous/Nonferrous Metal Cleaning
-
BONDERITE L-FG LS 2127
- Up to 1649 deg C Service
- Anti-Stick Non-Ferrous Tooling Coating
- Brush, Spray, or Dip Application
-
BONDERITE L-FM PRETREAT
- Heat-Treatment Scale Inhibition
- Lubricating Protective Forming Coating
- Fast-Drying Post-Treatment Descaling Aid
-
BONDERITE L-GP 460
- High-Purity Graphite Anti-Seize Lubricant
- High-Load Extreme-Pressure Lubrication
- Up to 538 deg C Service
-
BONDERITE M-CR 1001
- Clear Aluminum Chromate Conversion Coating
- Paint-Adhesion and Corrosion-Resistance Improvement
- Spray or Immersion Application
-
BONDERITE M-ED 1000
- Nickel Acetate-Based Sealing Process
- Reduced Smut, Powdering, and Yellowing
- Commercial and Selected Military Anodizing Seal Processes
-
BONDERITE M-FE 101
- One-Step Steel Cleaning and Phosphating
- Improved Paint Adhesion, Coating Durability, and Corrosion Resistance
- Steam Gun and High-Pressure Manual Applications
-
BONDERITE M-FE HMF-1080
- Heavy-Metal-Free Multi-Metal Clean/Phosphate Process
- Improved Paint Adhesion and Corrosion Resistance
- Multi-Metal Spray-Tunnel Pretreatment
-
BONDERITE M-MN LUBRITE 2
- Oil-Absorptive Phosphate Lubricating Coating
- Rapid Break-In and Reduced Scuffing
- Corrosion-Resistant Oil-Finishing Surface
-
BONDERITE S-FN 309
- Fast-Drying PTFE Dry-Film Lubrication
- Wood/Metal/Rubber/Plastic/Glass Surface Adhesion
- Spray/Brush/Dip/Roller Application Methods
-
BONDERITE S-FN 310A
- PTFE Dry-Film Low-Friction Release
- Longer Wear Life than Pure PTFE
- 149 deg C Low-Temperature Cure
-
BONDERITE S-FN 330
- Low-Friction Stick-Slip-Resistant Coating
- 500-Hour Salt-Spray/Humidity Resistance
- Up to 150 deg C Service
-
-
BONDERITE S-FN GP 1904
- PTFE/Graphite Dry-Film Lubricant
- Corrosion and Solvent Resistance
- Multi-Substrate Dry Lubrication
-
BONDERITE S-OT 310B
- PTFE Dry-Film Low-Friction Lubrication
- Oil, Solvent, and Chemical Resistance
- Metal and Rubber Coating Process
-
BONDERITE S-ST 5351
- Ambient-Temperature Aerospace Coating Removal
- Viscous Vertical-Surface Stripping
- MIL-R-81294 Aerospace Approval
-
BONDERITE S-ST 5668
- Aircraft Polyurethane/Epoxy Coating Removal
- Phenol-, Chromate-, Solvent-, and Acid-Free Formulation
- MIL-R-83936B Specification Compliance
-
ECCOBOND F112
- Low-Viscosity Controlled Dispensing
- Thermal-Shock and Impact Resistance
- Low-Stress No-Pistoning Connections
-
-
ECCOBOND F131
- Clear Fiber-Optic Assembly Epoxy
- Room-Temperature or Accelerated Heat Cure
- High-Tg Cured Epoxy
-
FREKOTE 710-NC
- Reduced Cleaning Frequency
- Thermally Stable Coating
- Compatible with Multiple Epoxy Molding Compounds (EMCs)
-
FREKOTE 720-NC
- Colorless Low-VOC Mold Release
- Solvent-Based Liquid Release Application
- Industrial Mold-Release Processing
-
FREKOTE 770-NC
- High-Cycle Semiconductor Mold Release
- Low-Residue Mold Release
- Epoxy-Molding-Compound Temperature Compatibility
-
FREKOTE 800-NC
- Repeat-Cycle Mold Release
- Low-Residue Mold Release
- Semiconductor Epoxy-Molding Temperature Compatibility
-
FREKOTE 815-NC
- Durable, Consistent Mold Release for High-Cycle Applications
- Precision Silicone Formulation Compatible with Semiconductor Molding
- Improved Yield Mold Release
-
FREKOTE AC4368
- Combined Mold Release and Conditioning
- Multi-Resin Molding Compatibility
- 5 to 10-Minute Solvent Evaporation
-
FREKOTE R-150
- Non-Flammable Mold Release Formulation
- Natural/Synthetic Rubber Release and Slip
- 60 to 200 deg C Mold Operation
-
-
FREKOTE EXITT-I
- High-Gloss Molded-Part Finish Retention
- Urethane-Elastomer Mold Release
- Wipe, Brush, or Spray Application
-
FREKOTE FMS
- Composite-Mold Microporosity Sealing
- High-Gloss Prepared Mold Surface
- 20-Minute Final-Coat Cure at 20 deg C
-
FREKOTE FMS-100
- Room-Temperature Mold-Sealer Cure
- Microporosity-Sealing Mold Preparation
- High-Gloss Release-Ready Surface
-
FREKOTE HMT
- Hot-Mold Direct Application
- Standalone or Touch-Up Release
- Multiple Releases without Transfer Buildup
-
FREKOTE PMC
- Polyester-Mold Wax Removal
- Multi-Soil Mold Cleaning
- FREKOTE Sealer/Release Surface Preparation
-
FREKOTE R100
- Multi-Cycle Mold Release
- Reduced Resin Adhesion to Molds
- Semi-Permanent Low-Residue Coating
-
FREKOTE R-120
- Semi-Permanent Rubber-Mold Release Coating
- 4-Minute 150 deg C Cure
- Multiple Releases with Low Transfer
-
-
-
LOCTITE 122S
- Thixotropic Application Control
- Non-Staining Mold Release Formulation
- Non-Flammable Mold Release Formulation
-
-
-
LOCTITE 242
- Medium-Strength Thread Retention
- Vibration-Resistant Fastener Threadlocking
- Thread Sealing Protection
-
LOCTITE 246
- High-Strength Thread Retention
- Vibration-Resistant Fastener Threadlocking
- One-Component Threadlocking System
-
LOCTITE 262
- One-Component Threadlocking System
- High-Strength Thread Retention
- Thixotropic Application Control
-
LOCTITE 263
- High-Strength Thread Retention
- Low-Viscosity Threadlocking Application
- High-Temperature Thread Retention
-
LOCTITE 266
- Oil-Tolerant Threadlocking Application
- High-Strength Thread Retention
- Thixotropic Application Control
-
LOCTITE 2701
- High-Strength Thread Retention
- Low-Viscosity Threadlocking Application
- Fluorescent Under UV Light
-
LOCTITE 271
- High-Strength Thread Retention
- Low-Viscosity Threadlocking Application
- Large Threaded-Fastener Locking
-
-
LOCTITE 277
- M25 Bolt/Stud Threadlocking
- High-Strength Thread Retention
- Medium-Viscosity Threadlocking Application
-
LOCTITE 290
- Wicking-Grade Thread Application
- Low-Viscosity Threadlocking Application
- High-Strength Thread Retention
-
LOCTITE 294
- Wicking-Grade Thread Application
- Low-Viscosity Threadlocking Application
- High-Strength Thread Retention
-
-
-
-
LOCTITE 4013
- Medium-Viscosity Cyanoacrylate Adhesive
- ISO 10993 Biocompatibility
- Disposable Medical-Device Assembly
-
-
-
LOCTITE 4081
- Very-Low-Viscosity Cyanoacrylate Adhesive
- Low-Odor Adhesive Cure
- Disposable Medical-Device Assembly
-
-
LOCTITE 410
- Rubber-Toughened Cyanoacrylate Adhesive
- Visible Cured Bondline
- Dynamic/Impact-Loading Adhesive Bonding
-
-
LOCTITE 415
- High-Viscosity Cyanoacrylate Adhesive
- Documented MIL-A-46050C/A-A-3097 Qualification
- Chemical and Environmental Resistance
-
LOCTITE 416
- High-Viscosity One-Part Cyanoacrylate
- Documented MIL-A-46050C/A-A-3097 Qualification
- Multi-Material Plastic/Rubber/Metal Bonding
-
LOCTITE 422
- High-Viscosity Cyanoacrylate Gel
- Transparent Cured Bondline
- Documented MIL-A-46050C/A-A-3097 Qualification
-
LOCTITE 426
- Toughened Structural Bonding
- Impact-Resistant Cyanoacrylate Bonding
- Gel-Consistency Bonding Placement
-
LOCTITE 444
- TAK PAK Accelerator Compatibility
- One-Component Cyanoacrylate Adhesive
- Documented A-A-3097 Qualification
-
LOCTITE 454
- Thixotropic Application Control
- High-Strength Structural Bonding
- Moisture-Cure Bonding Processing
-
-
-
LOCTITE 498
- General-Purpose Cyanoacrylate Adhesive
- Cured Thermal-Cycling Resistance
- Cured Humidity Resistance
-
LOCTITE 499
- Non-Sag Cyanoacrylate Gel
- One-Component Adhesive System
- Vertical/Overhead Adhesive Applications
-
LOCTITE 545
- One-Component Sealing System
- Thread Sealing and Locking
- Assembly Lubricity Sealant Formulation
-
-
LOCTITE 566
- Low-Strength Thread Sealing
- Vibration-Resistant Thread Sealing
- One-Component Sealing System
-
LOCTITE 567
- High-Lubricity Thread Assembly
- Anaerobic Thread Sealing
- High-Temperature Service Sealant Formulation
-
LOCTITE 569
- Low-Viscosity Sealing Application
- Vibration-Resistant Thread Sealing
- Broad Fluid Resistance
-
LOCTITE 592
- High-Lubricity Thread Assembly
- Immediate Low-Pressure Seal
- Elevated Temperature Fluid Resistance
-
LOCTITE 609
- High-Strength Cylindrical Retention
- Low-Viscosity Retention Application
- Vibration and Fluid Resistance
-
LOCTITE 620
- High Temperature Retention
- Gap-Filling Cylindrical Retention
- High Mechanical and Fluid Resistance
-
LOCTITE 648
- High-Strength Cylindrical Retention
- Metal Compatibility Cylindrical Retention
- Heat, Oil, and Contamination Resistance
-
LOCTITE 680
- High-Strength Cylindrical Retention
- Gap-Filling Cylindrical Retention
- Heat and Fluid Resistance
-
LOCTITE 962T
- Thixotropic Application Control
- High-Strength Joint Sealing
- Heat-Resistant Sealing Service
-
LOCTITE LB 8008 C5-A
- Copper-Based Anti-Seize Paste
- Galling Prevention in Assembly
- Against Corrosion and Oxidation Protection
-
-
-
LOCTITE CAT 15 LV
- Low-Viscosity Epoxy Hardener
- 120-Minute Working Time
- Rigid/Semi-Rigid/Flexible Epoxy Systems
-
LOCTITE CAT 17M-1
- Anhydride-Based Epoxy Hardener
- Non-Flammable Curing Agent
- Electronic/Industrial Resin Systems
-
LOCTITE CAT 21
- Low-Viscosity Polyoxyalkylene Amine Curative
- One-Hour Pot Life
- Large-Mass Epoxy Castings
-
LOCTITE CAT 23LV
- Low-Viscosity Polyamine Epoxy Catalyst
- Water-Soluble Curing Agent
- Low-VOC Amber Liquid
-
LOCTITE CAT 24LV
- Low-Viscosity Epoxy Curing Agent
- Long Epoxy Pot Life
- Low-Temperature Cured Epoxy Performance
-
-
LOCTITE CAT 43
- Liquid Polyamine Epoxy Catalyst
- Chemical-Resistant Cured Systems
- LOCTITE Encapsulant Compatibility
-
LOCTITE CAT 50-2
- Low-Viscosity Liquid Catalyst
- Dibutyltin Dilaurate Chemistry
- Consistent Catalytic Activity
-
LOCTITE CAT B97
- Low/Medium-Viscosity Epoxy Catalyst
- Encapsulation and Potting Systems
- Adhesion and Electrical Insulation
-
LOCTITE CAT9
- Modified Aliphatic Amine Hardener
- Chemical-Resistant Cured Epoxy
- -40 to 130 deg C Service
-
-
LOCTITE EDAG 1415M
- Silver-Filled Coating Application
- Low-Resistance Coating Application
- No Primer or Topcoat Required
-
LOCTITE EDAG 423SS
- Graphite-Filled Conductive Ink
- Low-Voltage Circuit Applications
- Broad Screen-Printing Equipment Compatibility
-
-
-
LOCTITE LB8009
- Steel Compatibility Paste Material
- Improved Clamp Load Consistency
- Non-Curing Assembly Formulation
-
LOCTITE LB8023
- Calcium-Sulfonate Grease Formulation
- High-Lubricity Thread Assembly
- Galvanic Corrosion Prevention
-
LOCTITE LB8034
- Synthetic PAO-Based Grease
- Long-Life Equipment Lubrication
- Water and Corrosion Resistance
-
LOCTITE LB8036
- Non-Metallic Grease Material
- High-Lubricity Thread Assembly
- 29C to 1093C Service Temperature
-
LOCTITE LB8040
- -43 deg C Freeze-and-Release Cooling
- Fast Penetrating Lubricant
- Corrosion-Protective Residual Film
-
LOCTITE LB8150
- Graphite/Aluminum Anti-Seize Lubricants
- Extreme-Pressure Additive Package
- MIL-PRF-907-H Requirement Compliance
-
LOCTITE LB8700
- Molybdenum Disulfide Anti-Seize Formulation
- Galling Prevention in Assembly
- Improved Clamp Load Consistency
-
LOCTITE LB8801
- Non-Curing Silicone Grease Formulation
- High and Low Temperature Stability
- Metal and Plastic Compatibility
-
LOCTITE MR5412
- Solvent-Based Neoprene Contact Adhesive
- Fast Air-Dry Tack
- Repositionable During Initial Assembly
-
LOCTITE SF 7840
- Biodegradable Aqueous Degreaser
- Hazardous-Solvent-Free Aqueous Formulation
- Non-Flammable Non-Caustic Cleaner
-
LOCTITE SF7090
- Accelerates Cure of Loctite Anaerobic Adhesives
- Solvent-Free Bonding Formulation
- Passive Metals and Inert Materials
-
LOCTITE SF712
- Loctite SF712 | Cyanoacrylate Adhesive Activator
- Fast Assembly Fixturing
- Low-Viscosity Bonding Flow
-
LOCTITE SF7452
- Cyanoacrylate Adhesive Cure Accelerator
- Fast Assembly Fixturing
- Low-Viscosity Bonding Flow
-
LOCTITE SF768
- Cyanoacrylate Residue Removal
- Very-Low-Viscosity Solvent Cleaner
- Surface Cleaning and Debonding
-
LOCTITE SICOMET 100
- 0.01 to 0.50 mm Gap Fill
- Fast Moisture-Cure Fixturing
- Strong Rubber/Plastic Adhesion
-
-
ABLESTIK 5074
- Flexible Dissimilar-Material Bonding
- Multiple Heat-Cure Options
- Reworkable Non-Conductive Film
-
ABLESTIK 642-1
- Extended 8-Hour Assembly Window
- Multiple Heat-Cure Schedules
- Low-Outgassing Assembly Bonding
-
ABLESTIK 64C
- Non-Silver Conductive Bonding
- Room-Temperature or Heat Cure
- Seawater-Exposure Assembly Fit
-
ABLESTIK CE 3511PHV
- Extended Dispensing Pot Life
- No-Bleed Conductive Placement
- Fast Hot-Plate Cure Option
-
ABLESTIK FS163
- Equal-Weight BIPAX Mixing
- Room-Temperature or Heat Cure
- Broad-Material Industrial Bonding
-
ABLESTIK G757HF-D
- Automotive Headlamp Lens Bonding
- Thixotropic Sag-Resistant Placement
- Flexible -40 to 150 deg C Operation
-
ABLESTIK ICP9000
- Semi-Sintering Power Die Attach
- Extended 16-Hour Work Life
- Thermal and Electrical Attach Path
-
BONDERITE C-AK 319
- Spray-or-Immersion Application Flexibility
- Effective Across Wide Concentration Range
- Multi-Metal Pre-Plating Surface Prep
-
BONDERITE C-AK 3878-LF-NC
- Chromate- and Chlorine-Free Formula
- Vapor-Degreasing Fluid Replacement
- Shop Soil and Cutting-Oil Removal
-
BONDERITE C-AK 4181-L
- Single-Step Rust and Corrosion Removal
- Immersion, Electrolytic, or Ultrasonic Use
- AMS-1379 Aerospace Specification Testing
-
-
BONDERITE C-AK 5578-L
- Combined Cleaning and Titanium Etching
- Pre-Bonding Surface Etch Preparation
- Concentration-Controlled Process Flexibility
-
BONDERITE C-IC 4104
- Nitric Acid Descaling Enhancement
- Multi-Alloy Pickling Compatibility
- Alloy-Tailored Bath Formulation
-
BONDERITE C-MC 5884
- MIL-C-85704C Type I Qualification
- GE and Pratt and Whitney Engine Listings
- Ash-Free Water-Miscible Cleaning
-
BONDERITE C-SO 4460
- BMS 11-7G Wipe-Solvent Qualification
- Rapid Residue-Free Evaporation
- Multi-Metal Pretreatment Wiping
-
BONDERITE L-AD 42
- Organosilicone Surfactant Foam Control
- Free-Rinsing Low-Residue Chemistry
- Polymer, Adhesive, and Latex Foam Control
-
BONDERITE L-GP-D148A
- PTFE Dry-Film Lubricant Formation
- Spray-Viscosity Thinning Compatibility
- Room-Temperature Cure with Heat Acceleration
-
BONDERITE M-CR 120
- Two-Step Aluminum Deoxidizing and Coating
- Manual Brush-Applied Aluminum Treatment
- Pre-Portioned Two-Component Kit Packaging
-
BONDERITE S-AD 103
- Acid-Bath Corrosion Inhibition
- Direct Liquid Addition to Acid Baths
- Industrial Metal-Cleaning Bath Support
-
ECCOBOND LUX OGR146TUV
- UV and Shadow-Area Thermal Cure
- Low-Refractive-Index Optical Bonding
- Extended 91-Day Working Window
-
FREKOTE 710-LV
- Room-Temperature Semi-Permanent Release
- High-Slip High-Gloss Finish
- Controlled Two-Coat Application
-
FREKOTE PUR-100
- Water-Based Non-Flammable Release
- Multiple Releases Per Application
- Paint-Ready Molded Parts
-
LOCTITE 079
- Serviceable Low-Strength Thread Locking
- One-Part Anaerobic Application
- Purple Visual Identification
-
-
-
LOCTITE 087
- High-Strength Coarse-Thread Retention
- 11.3 to 28.3 N m Prevail Torque
- One-Part Heat-Assisted Disassembly
-
LOCTITE 220
- Wicking Preassembled Threadlocking
- Low-Strength Hand-Tool Removal
- UV-Visible Application Inspection
-
LOCTITE 222MS
- Low-Migration Thixotropic Application
- Easy Hand-Tool Disassembly
- Small-Fastener Threadlocking Control
-
LOCTITE 2422
- High-Temperature Threadlocking Paste
- Thixotropic Paste Application
- Serviceable Medium-Strength Locking
-
-
LOCTITE 2620
- Elevated-Temperature Threadlocking Paste
- Thixotropic Paste Placement
- Medium-to-High Fastener Retention
-
-
-
-
LOCTITE 380
- Rubber-Toughened Shock Resistance
- Black Bondline Identification
- Fast Multi-Substrate Fixturing
-
LOCTITE 4014
- Very-Low-Viscosity Precision Bonding
- Fast Mixed-Material Fixturing
- Heat-Conditioned Bond Strength
-
LOCTITE 408
- Low-Odor Low-Blooming Bonding
- Very-Low-Viscosity Joint Wetting
- Rapid Porous-Material Fixturing
-
LOCTITE 420
- Very-Low-Viscosity Capillary Bonding
- Fast Close-Fitting Assembly
- Broad Metal-Plastic-Rubber Bonding
-
LOCTITE 4210
- Elastomer-Toughened Impact Resistance
- Low-Viscosity Thin-Gap Bonding
- Fast Multi-Substrate Fixturing
-
LOCTITE 425
- Fast Plated-Fastener Fixturing
- Low-Strength Serviceable Retention
- Pre- or Post-Applied Locking
-
-
-
LOCTITE 431
- Medium-Viscosity Application Control
- Rapid Multi-Material Bonding
- Strong Shear-Oriented Performance
-
LOCTITE 435
- Rubber-Toughened Peel Resistance
- Low-Viscosity Rapid Bonding
- Porous-Material Bonding Range
-
LOCTITE 438
- Black Rubber-Toughened Bonding
- Enhanced Shock and Peel Resistance
- Low-Viscosity Multi-Material Assembly
-
LOCTITE 460
- Low-Odor Low-Blooming Cure
- Very Fast Porous-Substrate Fixturing
- Low-Viscosity Vapor-Controlled Bonding
-
LOCTITE 493
- Very-Low-Viscosity Capillary Bonding
- Fast Metal-Focused Fixturing
- Broad Rubber-Plastic Bonding
-
LOCTITE 542
- Low-Viscosity Fine-Thread Sealing
- Anaerobic One-Part Application
- Medium-Strength Serviceable Retention
-
LOCTITE 571
- Medium-Viscosity Tapered-Thread Sealing
- Anaerobic One-Part Retention
- Fluid-Exposure Strength Retention
-
LOCTITE 635
- High-Strength Cylindrical Retention
- Medium-Viscosity Application Control
- Anaerobic One-Part Metal Cure
-
LOCTITE 641
- Serviceable Medium-Strength Retention
- Controlled Medium-Viscosity Flow
- Anaerobic One-Part Metal Cure
-
LOCTITE 662
- Anaerobic-and-UV Dual Cure
- Fast Exposed-Bead Fixturing
- High-Strength Cylindrical Retention
-
-
LOCTITE 8060
- High-Temperature Anti-Seize Protection
- Controlled Stick Application
- Measured Assembly Torque Behavior
-
LOCTITE 88
- Organic Air-Release Performance
- Multi-Resin Formulation Scope
- Vacuum De-Airing Process Support
-
LOCTITE ECI1016
- High-Speed Rotary Screen Printing
- Low-Resistance Silver Conductive Traces
- Two-Minute Hot-Air Drying
-
LOCTITE EDAG 33RO65A
- High-Speed Conductive Printing
- Graphite-Polyimide Temperature Stability
- Low-Resistance Printed Conductivity
-
LOCTITE HC 9872.1
- Low-density syntactic core costruction
- Excellent moisture resistance
- Compatible with 350°F epoxy prepregs
-
LOCTITE LB8017
- Multi-Method Dry-Film Application
- 400 deg C Sliding Service
- 1315 deg C Anti-Seize Range
-
LOCTITE LB8504
- Non-Metallic Conductive Anti-Seize
- 482 deg C Operating Range
- 0.13 Steel Fastener Torque Coefficient
-
LOCTITE NS5109
- High-Temperature Flexible Sealing
- High-Pressure Sealing up to 34 MPa
- One-Part No-Mix Application
-
LOCTITE PC6231
- Rapid 90-Minute Full Cure
- Self-Leveling Low-Viscosity Fill
- 10-15% Joint Movement Capability
-
LOCTITE SF7070
- Low-Viscosity Precision Cleaning
- 5-20 Minute Drying Window
- Spray, Wipe, or Immersion Use
-
-
LOCTITE SF7649
- Thirty-Day On-Part Life
- Low-Temperature Cure Acceleration
- Brush, Spray, or Pre-Applied Use
-
-
-
-
-
-
LOCTITE 4541
- Non-Drip Vertical Application
- Fast Porous-Material Fixturing
- Multi-Material Instant Bonding
-
-
-
-
ABLESTIK 2600BT
- 20 W/(m K) Thermal Conductivity
- 0.001 ohm-cm Volume Resistivity
- 40 ppm/deg C CTE Below Tg
-
-
-
ABLESTIK 8177
- 4-Minute 130 deg C Cure
- 3.0 W/(m K) Thermal Conductivity
- 0.0001 ohm cm Volume Resistivity
-
ABLESTIK 958
- Conductive And Non-Conductive Variants
- Stress-Absorbing Die-Attach Options
- 958-7 17 N/mm^2 Gold Lap Shear
-
ABLESTIK C990
- Silver-Filled Conductive Die Attach
- Stamping-Compatible C 990 333
- C 990 333 20-Second Hot-Plate Cure
-
ABLESTIK E3503-1
- Thin-Bondline Thermal Adhesive
- Electrically Non-Conductive Thermal Adhesive
- Low-Temperature Heat Cure
-
-
ABLESTIK ECF 550X
- Three-Axis Electrical Conductivity
- 2.1 W/(m K) Thermal Conductivity
- 3-Day Work Life at 25 deg C
-
-
LOCTITE ABLESTIK XCP 3302NS
- 8-Hour Open Time After Dispense
- 1.75 W/(m K) Thermal Conductivity
- 0.0006 ohm cm Volume Resistivity
-
BONDERITE C-AK 212
- Silicate-Free Aluminum Cleaning
- Low-Etch Oil and Oxide Removal
- Spray or Immersion Processing
-
BONDERITE C-AK 305
- Low-Foam Metal Strip Cleaning
- Continuous Spray-Plant Processing
- Controlled Alkaline Etching
-
BONDERITE C-AK 4848-257
- Aerospace Surface Preparation
- Controlled Flood-and-Wipe Cleaning
- 15-Minute Room-Temperature Drying
-
BONDERITE C-AK 6751-L
- Multi-Soil Metal Cleaning
- Room-Temperature Water Rinsing
- 30 to 60 deg C Operation
-
BONDERITE C-AK 6871
- Water-Dilutable Alkaline Concentrate
- Painted or Unpainted Aircraft Cleaning
- Spray or Foam Application
-
BONDERITE C-AK 9045-6
- Ready-to-Use Carbon Removal
- 40 to 60 deg C Operation
- Mechanically Agitated Tank Cleaning
-
-
-
BONDERITE C-MC 6802
- Platter Wax Removal
- All-Metal Cleaning Capability
- Chlorinated Hydrocarbon-Free Formulation
-
BONDERITE C-SO 263
- Paint Equipment Residue Removal
- Paint, Oil, and Grease Dissolution
- Liquid Solvent Cleaning
-
-
BONDERITE L-GP 39SY201
- Visible Gear Alignment Pattern
- Easy Brush Application
- Homogeneous Lump-Free Paste
-
BONDERITE L-GP 6041 CR
- Extended Indoor Corrosion Protection
- Non-Tacky Protective Film
- Dip Spray or Hand Application
-
BONDERITE L-MR 9103
- Clear-View Machining Dilution
- Oil-Rejecting Coolant Operation
- Low-Foam Ferrous Metalworking
-
BONDERITE M-AD 131
- Zinc-Phosphate Bath Acceleration
- Near-Neutral pH Profile
- Odorless Liquid Process Additive
-
BONDERITE M-AD 315
- Controlled Silicofluoride Bath Adjustment
- Defined 1.46 kg Addition Rate
- Immersion or Spray Phosphating
-
BONDERITE M-AD 500
- Dual Zinc and Iron Bath Adjustment
- Controlled 1:4 Pre-Dilution
- Stepwise pH Correction
-
BONDERITE M-AD40
- Strongly Alkaline Pretreatment Cleaning
- Complete Water Solubility
- Defined Low-Temperature Storage Boundary
-
BONDERITE M-FE 1070
- One-Step Cleaning and Conversion
- Uniform Non-Metallic Phosphate Coating
- Spray or Immersion Processing
-
BONDERITE M-FE 330SW
- Three-Function Aluminum Pretreatment
- Defined 60 to 120 deg F Window
- Explicit High-Copper Alloy Exclusion
-
BONDERITE M-NT 601
- Phosphate-Free Conversion Processing
- Spray or Immersion Application
- Multi-Metal Paint Preparation
-
BONDERITE M-ZN 1083
- Spray-Process Metal Conversion
- Industrial-Scale Drum Supply
- Exact IDH 596526 Grade Mapping
-
BONDERITE S-AD 3305
- Non-Foaming Pickling-Bath Inhibition
- Scale Removal Without Rate Loss
- Reduced Acid Consumption
-
BONDERITE S-AD 50
- Hydrochloric-Acid Pickling Inhibition
- Non-Foaming Liquid Bath Additive
- 1 to 6 g/L Process Concentration
-
BONDERITE S-FN 329
- Room-Temperature Dry-Film Cure
- 0.06 to 0.09 Static Friction
- Spray, Dip, or Brush Application
-
BONDERITE S-FN 6767
- Oil-Based Corrosion Protection
- Combined Lubrication and Rust Prevention
- Liquid Protective-Lubricant Format
-
BONDERITE S-ST 6776
- Dip and High-Cling Variant Options
- Epoxy and Polyurethane Paint Removal
- Methylene-Chloride-Free Stripping Chemistry
-
BONDERITE S-ST 6776-LO
- Vertical and Overhead Surface Cling
- Ready-to-Use Spray or Manual Application
- Epoxy and Polyurethane Paint Removal
-
BONDERITE S-ST 6813 E
- Multi-Coat Aerospace Paint Removal
- Vertical and Overhead Surface Cling
- Cold-Water Rinse Removal
-
BONDERITE S-ST 6930
- Hydrogen-Peroxide-Activated Paint Removal
- Vertical and Overhead Surface Cling
- High-Pressure Water-Rinse Removal
-
-
ECCOBOND LUX A4021T
- 365 nm UV or 470 nm Visible Cure
- 1.3% Linear Cure Shrinkage
- 1.589 Refractive Index at 589 nm
-
FIXMASTER FLEX 80
- Two-Part Black Urethane
- Casting and Rebuilding Parts
- Corrosion, Wear, and Impact Exposure
-
-
FREKOTE C-210
- Above 60 deg C Hot-Mold Touch-Up
- Ready-to-Use No-Mix Emulsion
- Spray, Brush, Wipe, or Dip
-
-
-
-
HST TITRATING SOLUTION 18
- Potassium Permanganate Titrating Solution
- Exact IDH 592429 Identity
- Process Bath Concentration Control
-
LOCTITE 190828
- Rapid Humidity-Cure Bonding
- Thermal-Cycling-Resistant Cyanoacrylate Adhesion
- Multi-Substrate Instant Assembly
-
LOCTITE 232
- Lubricated Heavy-Fit Assembly
- Medium-Strength Anaerobic Retention
- Steel Press-Fit Shear Performance
-
LOCTITE 2432
- Activation-Free Stainless Threadlocking
- Low-Migration Thixotropic Application
- Controlled Halogen and Sulfur Content
-
LOCTITE 279
- High-Strength Thread Retention
- Threaded and Cylindrical Bonding
- Wide-Temperature Threadlocking Range
-
LOCTITE 2892
- High-Viscosity Flange Gap Filling
- Resilient Flange-Movement Sealing
- Manual or Screen-Print Application
-
LOCTITE AA 3060
- Rapid 30-120-Second Steel Fixture
- Thixotropic 1:1 External Mixing
- High-Impact Magnet Bonding
-
LOCTITE PE 3162
- Dedicated PE Hardener Component
- Amber Liquid Component Identification
- Estimated Zero VOC Content
-
LOCTITE 3607
- Pin-Transfer Dot Placement
- Humidity-Tolerant Open-Bath Dispensing
- 150 to 180-Second Heat Cure
-
-
LOCTITE 3627
- High-Speed SMD Dotting
- Dual Syringe-Stencil Processing
- Lead-Free Wave-Solder Compatibility
-
-
LOCTITE 402
- Low-Viscosity Instant Assembly
- Fast Multi-Substrate Fixturing
- Heat and Humidity Resistance
-
-
-
LOCTITE 4203
- Elastomer-Toughened Heat-Resistant Bonds
- Fast Multi-Substrate Fixturing
- Impact and Peel Resistance
-
-
LOCTITE 4305
- Rapid Dual-Cure Surface Bonding
- Fast 5-Second Tack-Free Response
- Plastics, Rubbers and Metals Bonding
-
LOCTITE 4471
- Fast Difficult-Surface Fixturing
- Uniform-Stress Assembly Bonding
- Porous and Plated Surface Bonding
-
LOCTITE 4981
- Heat-Resistant Instant Bonding
- Thermal-Cycling and Humidity Resistance
- Rapid Multi-Substrate Fixturing
-
LOCTITE 50H
- Low-Viscosity Instant Bonding
- Colorless Assembly Bonding
- Fast Dissimilar-Substrate Bonding
-
LOCTITE 5113
- Immediate Moderate-Pressure Sealing
- Wide -51 to 149 deg C Range
- Metal Pipe and Flange Sealing
-
-
LOCTITE 536
- Low-Torque Thread Disassembly
- Anti-Galling Metal Thread Lubricity
- Immediate Moderate-Pressure Sealing
-
LOCTITE 5452
- Particle-Free Hydraulic Sealing
- Large-Diameter Thread Coverage
- Hand-Tool Fitting Disassembly
-
LOCTITE 564
- Lubricated Pipe Thread Assembly
- High-Viscosity Thread Sealing
- Low-Strength Anaerobic Locking
-
LOCTITE 565
- Controlled-Locking Thread Sealing
- High-Pressure Pipe Sealability
- High-Viscosity Paste Application
-
LOCTITE 572
- Medium-Strength Thread Locking
- Thixotropic Migration Control
- Metal Pipe and Fitting Sealing
-
LOCTITE 5770
- High-Temperature Steam Thread Sealing
- High-Pressure Steel Joint Sealing
- Medium-Strength Anaerobic Locking
-
LOCTITE 5772
- Activator-Free Stainless Steel Sealing
- Low-Halogen Sensitive-Metal Formulation
- UV-Fluorescent Product Identification
-
LOCTITE 603
- Low-Viscosity Cylindrical Component Retaining
- High-Strength Steel Component Retention
- Shock-and-Vibration Assembly Retention
-
LOCTITE 661
- Dual Anaerobic and UV Cure
- Low-Viscosity Shaft Component Retention
- High-Strength Steel Component Retention
-
LOCTITE LB 8012
- 65% Molybdenum Disulfide Content
- High-Temperature Anti-Seize Service Range
- Low-Friction Threaded Fastener Assembly
-
-
LOCTITE CAT 28
- Low-Viscosity Catalyst Handling
- Long-Pot-Life System Processing
- STYCAST 2651MM Catalyst Pairing
-
-
LOCTITE DRI 513HV
- High-Temperature Thread Sealing
- Re-Adjustable Threaded Assemblies
- Dry-Film Non-Curing Seal
-
LOCTITE ECI 8120
- Screen-Printable Flexible Heater Ink
- Self-Regulating Low-Voltage Heating
- PET PEN and PI Printing
-
LOCTITE EDAG 6017SS
- Flexible Screen-Printed Conductive Features
- Low-Temperature Heat-Dry Processing
- Resistors, Heaters, Sensors and ESD
-
-
LOCTITE HD 8340RD
- One-Component Moisture-Cure Processing
- Polyurethane Panel-Lamination Format
- Sandwich-Panel Evaluation Fit
-
LOCTITE IS 5110
- Low-Viscosity Leak-Path Impregnation
- Water-Rinsable Post-Impregnation Cleanup
- Anaerobic Sealing Inside Porosity
-
LOCTITE LB 771
- Nickel-Based High-Temperature Anti-Seize
- Galling and Corrosion Protection
- Threaded and Press-Fit Assembly Use
-
LOCTITE LB 8007
- Copper/Graphite Anti-Seize Protection
- High-Temperature Threaded Assembly Service
- Lower-Friction Threaded Assembly
-
LOCTITE LB 8013
- Metal-Free High-Purity Anti-Seize
- Calcium Oxide/Graphite Lubrication
- High-Temperature Thread Protection
-
LOCTITE LB 8014
- 400 deg C Anti-Seize Range
- Metal-Free White Formulation
- Stainless-Steel Galling Protection
-
-
LOCTITE LB 8044
- 398 deg C Anti-Seize Range
- Aluminum Hardware Anti-Seize
- 0.15 Tested Torque Coefficient
-
LOCTITE LB 8209
- PFPE/PTFE Chemical-Environment Grease
- 810 cSt PFPE Base Oil
- -26 to 260 deg C Operating Range
-
-
LOCTITE LB 8423
- 19.8 kV/mm Dielectric Strength
- 2.6 x 10^15 ohm cm Resistivity
- -55 to 204 deg C Operating Range
-
LOCTITE LB 8507
- Nickel-Graphite Anti-Seize Blend
- Aerosol, Liquid, or Paste Form
- 12 oz Package Configuration
-
-
-
-
-
-
-
LOCTITE N-1000
- Up to 982 deg C Operating Range
- Low-Contaminant Copper-Graphite Formula
- 0.17 Steel-Fastener Torque Coefficient
-
LOCTITE N-5000
- -29 to 1315 deg C Range
- Low-Contaminant Nickel-Graphite Formula
- 0.18 Stainless-Fastener Torque Coefficient
-
-
LOCTITE PC 7202
- Self-Leveling Machinery Chocking
- 10 to 15-Minute Working Window
- 110 N/mm^2 Cured Compressive Strength
-
LOCTITE PC 7210
- 30-Minute 25 deg C Working Life
- 35 N/mm^2 Steel Lap Shear
- Composite Pipe and Tank Repair
-
LOCTITE PC 7227
- Ultra-Smooth Brushable Ceramic Coating
- 92 um Vertical Sag Resistance
- 100 deg C Dry Service
-
-
-
-
LOCTITE PC 7303
- 4:1 Resin-to-Hardener Mixing
- 148 deg C High-Temperature Post-Cure
- -29 to 232 deg C Dry Service
-
LOCTITE PC 7317
- Small-Bead Fine-Abrasion Protection
- 6-Hour 25 deg C Cure
- 103 N/mm^2 Compressive Strength
-
-
-
-
LOCTITE PC9410
- 3 to 11 Minute Initial Set
- -25 to 45 deg C Placement Range
- 17 to 21 N/mm^2 Strength After 2 Hours
-
LOCTITE PC9422
- 460 mm Maximum Grout Depth
- 285-Minute Working Life
- 95 N/mm^2 Cured Compressive Strength
-
-
-
-
-
-
LOCTITE UR 3371
- 40-Minute Skin-Over Time
- -30 to 80 deg C Service Range
- More Than 300% Cured Elongation
-
LOCTITE UR 8331
- One-Part Moisture-Cure Polyurethane
- Solvent-Free Laminating Adhesive
- Multi-Material Sandwich-Panel Bonding
-
-
LOCTITE UR 8543RD
- 22-Minute Open-Time Lamination
- No-Mix Bead or Trowel Application
- Untreated Aluminum Frame Adhesion
-
LOCTITE ABLESTIK 8008HT
- Thermally conductive
- Low modulus
- Stencil printing
-
-
-
-
-
LOCTITE ABLESTIK EMI 3620FA
- Compartment EMI Shielding
- No popcorning and delamination
- For gap, hole and trench filling
-
-
-
-
-
-
-
-
-
LOCTITE ABLESTIK EMI 8660S
- Conformal EMI shielding
- Excellent adhesion on EMC, Au, Ag
- Spray, Print, Dispense
-
-
-
LOCTITE ABLESTIK 2025D
- Excellent dispense capabilities
- For mother die in array packaging
- 260ºC reflow capability for Pb-free applications
-
-
-
-
LOCTITE ABLESTIK 2902
- Electrically conductive
- Thermally conductive
- Ceramic, metal, glass and plastic substrates
-
LOCTITE ABLESTIK ATB F150E
- 50um
- Non Conductive
- Wafer lamination and Chip on chip
-
-
ECCOBOND FP4530SF
- Approximately 25 um Flip-Chip Gap
- Blue-to-Green Cure Indication
- 8-Minute Snap Cure at 160 deg C
-
-
-
-
LOCTITE ABLESTIK 2025DSI
- With Spacers
- For mother die in array packaging
- 260ºC reflow capability for Pb-free applications
-
-
ECCOBOND UF3800
- 375 mPa s Viscosity at 25 deg C
- Cure Time of at Least 8 Minutes at 130 deg C
- CSP/BGA Underfill Rework Procedure
-
-
LOCTITE 3508NH
- Reworkable
- Reflow curable
- Improves mechanical reliability
-
-
-
-
-
-
-
-
LOCTITE ABLESTIK 50298
- Two components
- Nickel filled
- Alternative to Silver filled
-
-
-
-
-
-
-
-
-
-
-
-
-
-
-
LOCTITE ABLESTIK CDF 815P
- Electrically conductive
- Thermally conductive
- QFN, SOIC, SO
-
-
-
-
LOCTITE ABLESTIK ACP 3122
- Conductive only in z axis
- Anisotropic electrically conductive
- Low temperature cure
-
LOCTITE ABLESTIK 5025E
- Thin, uniform bondline control
- Electrically conductive in x,y,z axes
- Excellent electrical and thermal conductivity
-
-
LOCTITE 3536
- Reworkable Epoxy Underfill
- Rapid Low-Temperature Cure
- Low-Thermal-Stress Underfill Material
-
-
-
-
LOCTITE EDAG AV458 E&C
- Conductive
- Compatible with PC and Polyester
- Good flexibility
-
-
LOCTITE ABLESTIK CE3103WLV
- Pb Free alternative to solder
- Compatible with non noble metals
- Optimized for dispensing
-
LOCTITE EDAG PD 056 E&C
- Flexible coating
- Infrared cure
- High speed rotogravure
-
-
LOCTITE ABLESTIK CE3104WXL
- Pb Free alternative to solder
- Electrically conductive
- Optimized for printing
-
LOCTITE EDAG PF 021 E&C
- Encapsulating Photopolymer
- Prevents Silver migration
- Fast UV Cure
-
LOCTITE ABLESTIK ECF 564A
- Electrically conductive
- Excellent thermal conductivity
- Passes Mil 5011 and NASA outgassing
-
LOCTITE ABLESTIK NCF 218
- Non conductive Underfill film
- Enables fine pitch, narrow gap Cu pillar
- TSV, Die to die & Die to substrate
-
-
LOCTITE ABLESTIK ECF 564AHF
- High flow version of 564A
- Excellent thermal conductivity
- Passes Mil 5011 and NASA outgassing
-
-
-
-
-
-
-
LOCTITE ABLESTIK NCF 234
- Non-conductive Underfill Film
- Enable fine pitch, narrow gap Cu Pillar
- Pb-free & low κ
-
-
-
LOCTITE ABLESTIK A329-1
- Class F (155°C)
- Insulating applications
- Resistance to water, freon, solvents etc
-
-
-
-
LOCTITE ABLESTIK 71-1
- High bond strength
- High purity
- Electrically conductive
-
-
-
-
LOCTITE TC8M
- High Thermal-Conductivity Silicone Grease
- Electrical-Insulation Thermal Grease
- Corrosion-Protective Thermal Grease
-
LOCTITE ECCOBOND FP4502
- One component
- Low CTE
- No-clean flux compatible
-
-
-
LOCTITE ABLESTIK 71-1N
- Degassed 71-1
- Polyimide resin
- High adhesion
-
-
-
-
-
-
-
-
LOCTITE ABLESTIK ICP 3535M2
- Adhesion stability
- Pb free alternative to solder
- Excellent for Sn terminated components
-
-
-
-
LOCTITE ABLESTIK ICP 4000
- High temperature performance
- Excellent electrical conductivity
- Flexible and low stress
-
-
-
-
-
-
-
-
LOCTITE AA 3103
- UV/Visible-Light Adhesive Cure
- High-Adhesion Adhesive Bonding
- Polycarbonate Bonding Application
-
-
-
-
-
-
LOCTITE 3104
- UV/Visible-Light Adhesive Cure
- Direct PVC-to-Polycarbonate Bonding
- Low-Viscosity Adhesive Application
-
-
-
-
-
-
-
-
LOCTITE 383
- High-Viscosity Placement Control
- 0.602 W/(m K) Thermal Bonding
- One-Component Thermal Bonding System
-
-
-
-
LOCTITE 384
- 0.757 W/(m K) Thermal Conductivity
- Room-Temperature Activator Cure
- Controlled Medium-Strength Bonding
-
-
LOCTITE ECCOBOND NCP5209
- Non conductive
- Excellent protection of electrical joints
- Small assembly gaps and tight pitches
-
-
LOCTITE 4031
- Low-Odor Cyanoacrylate Adhesive
- Low-Blooming Adhesive Cure
- Medical-Device Bonding Applications
-
TECHNOMELT 1942
- 30-Second Assembly Open Time
- Wood and Multi-Plastic Bonding
- High-Elongation Hot-Melt Performance
-
-
-
Loctite SI 5970 - Gasketing Sealant
- One-Component Thixotropic RTV Silicone
- 25-Minute Tack-Free Time
- Oil-Resistant Sheet-Metal Gasketing
-
-
-
-
-
-
LOCTITE ABLESTIK 8322A
- Minimal resin bleed
- Large device bonding
- Accurate bondline control
-
LOCTITE ECCOBOND UF 3578
- Fast heat-cure adhesive designed for underfill and fixture applications
- Thixotropic and fluorescent for controlled flow and optical inspection
- Reflow-compatible for SMT processes
-
LOCTITE 414
- Low-Viscosity General Bonding
- Fast Rubber and Plastic Fixturing
- Strong Thin-Gap Metal Bonds
-
-
-
-
-
-
-
LOCTITE TCP7000
- Stencil-Printable Phase-Change Layer
- No Pump-Out or Dry-Out
- Reworkable Silicone-Free Interface
-
-
-
-
LOCTITE AA 3035
- Low Energy Plastic Bonding
- Fast Room-Temperature Bonding Cure
- Multi-Substrate Durability Acrylic Bonding
-
LOCTITE EIF1000
- Phase-Change Surface Conformability
- Kapton-Based Electrical Isolation
- Residue-Free Pad Replacement
-
-
BERGQUIST SIL PAD TSP 1600S
- 0.61 deg C in^2/W Thermal Impedance
- Electrical-Insulation Thermal Interface
- Compliant Fiberglass-Reinforced Low-Pressure Thermal Pad
-
-
-
-
BONDERITE C-AD-ETCH
- Smooth Aluminum Etching for Anodizing
- Adjustable Etch-Factor Additive Concentration
- Concentrated Sodium-Hydroxide Etchant Additive
-
-
LOCTITE AA 330
- Multi-Material Urethane Bonding
- One-Component Application Urethane Bonding
- High-Strength Structural Bonding
-
BERGQUIST TGF 3600
- 3.6 W/m-K Thermal Conductivity
- Sixty-Minute Application Window
- Soft Conforming Gap Fill
-
LOCTITE TCF1000
- Pressure-Responsive Thermal Impedance
- Reworkable Residue-Free Removal
- Silicone-Free Phase-Change Interface
-
-
BONDERITE M-CR 1132 AERO TOUCH-N-PREP PEN
- Ready-to-Use Touch-N-Prep Pen
- No-Rinse Dry-in-Place Processing
- Modifiable Felt-Tip Applicator
-
LOCTITE SI 5900
- At Least 100-Second Blow-Out Resistance
- At Most 0.2 mm ISO 7390 Flow
- At Least 400% Cured Elongation
-
LOCTITE AA 3311
- High Speed Light Cure
- Multi-Substrate Urethane Bonding
- Medical Devices Urethane Bonding
-
-
-
-
-
-
LOCTITE SI 5040
- One-Component Sealing System
- Non-Corrosive Sealing Formulation
- Self-Leveling Flowable Placement
-
BONDERITE M-CR 1200S
- MIL-DTL-5541 Qualified Aluminum Coating
- Immersion, Spray, or Brush Application Flexibility
- Wide-Range Bath Operating Window
-
-
LOCTITE ECCOBOND UF 9000AE
- Low die warpage
- Best large die underfill
- 260°C reflow capability for Pb- free, low-k applications
-
LOCTITE AA 3412
- High-Strength Structural Bonding
- Non-Sag Placement Control
- Fast Room Temperature Curing
-
-
LOCTITE SI 5699
- One-Component Oxime RTV Silicone
- Non-Corrosive Flange Sealant
- Rigid-Flange Sealing Applications
-
BONDERITE M-CR 1201
- MIL-DTL-81706 Brush-Application Approval
- Ready-to-Use Without Titration or Adjustment
- Integral Gold-to-Tan Aluminum Coating
-
-
-
BONDERITE M-CR 1500
- Transparent Chromate Conversion Coating
- Immersion, Spray, or Brush Application
- Documented MIL-DTL-81706/MIL-DTL-5541 Qualification
-
LOCTITE AA 3494
- UV/Visible-Light Adhesive Cure
- 10-Second or Faster Fixture
- Electrically Insulating Acrylic Adhesive
-
-
LOCTITE SI 593
- Non-Slumping Sealant Formulation
- Adhesion and Flexibility
- Seals Out Moisture and Contaminants
-
-
BONDERITE M-CR 1600
- Hexavalent Chromate Conversion Coating
- Immersion or Spray Processing
- MIL-DTL-81706A/BAC 5719 Approval
-
-
LOCTITE SI 5920
- One-Component Sealing System
- Non-Corrosive Sealing Formulation
- Thixotropic Application Control
-
-
-
LOCTITE DA 100
- Sn91.5/Sb8.5 - Pb free 92A Alloy
- Semiconductor die attach
- Excellent dispense capabilities
-
BONDERITE M-CR 600
- Ready-to-Use Chromate Conversion Coating
- Aluminum Corrosion Protection and Paint Adhesion
- QPL-81706 Aerospace Qualification
-
-
LOCTITE SI 596
- Enhances Load Bearing
- Reduced-Migration Sealing Formulation
- Good Temperature Resistance
-
-
LOCTITE GC 10
- SAC 305 - No refrigeration
- PCB Assembly
- Stencil Printable
-
LOCTITE FP4804 | Epoxy Underfill
- Good flowability
- Low CTE/modulus (reduced stress)
- No resin bleed out on glass
-
BONDERITE M-CR 871
- One-Part Dry-in-Place Conversion Coating
- Corrosion Protection and Paint Adhesion
- Touch-N-Prep Aerospace Repair Application
-
LOCTITE AA 3924
- Fast UV/Visible-Light Fixture
- Sterilization-Resistant Cured Bondline
- Medical-Device Assembly Bonding
-
LOCTITE GC 18
- SAC 305 - No refrigeration
- Low voiding
- Stencil Printable
-
-
BONDERITE M-CR-T5900
- Trivalent-Chromium Corrosion-Resistant Conversion Coating
- MIL-DTL-81706/5541 Type II Qualification
- Immersion or Pressure-Spray Processing
-
LOCTITE AA 3974
- Rapid UV/Visible-Light Fixture
- Thermal-Cycling-Resistant Cured Adhesive
- Potting/Sealing/Bonding Assembly Applications
-
LOCTITE GC 50
- SAC 305 - No refrigeration
- Low voiding
- Fine nozzle Jet dispensing
-
-
BONDERITE M-ED 720
- Targeted Hard-Coat Bath Addition
- Sulfuric-Acid Anodizing Integration
- Defined Bath-Stage Process Role
-
-
LOCTITE HF 212
- 90ISC and 97SC Alloys
- Halogen free
- Stencil Printable
-
-
BONDERITE M-NT 1455
- Chromium-Free Conversion Treatment
- Dry-in-Place Conversion Processing
- Multi-Metal Pretreatment Coverage
-
-
LOCTITE AA H8000
- Fast Assembly Fixturing
- Impact-Resistant Methacrylate Bonding
- Minimal Surface Preparation Needed
-
BONDERITE M-NT 1455-W
- Wash-Free Wipe-On Pretreatment
- Multi-Metal Surface Preparation
- Corrosion-Protective Paint Base
-
-
LOCTITE LF 318
- 90iSC Alloy
- Automotive reliability qualified
- Stencil Printable
-
Loctite STYCAST 2651-40W1
- Epoxy Potting and Encapsulation Resin
- Room-Temperature Encapsulation Cure
- 0.5 W/(m K) Thermal Encapsulation
-
BONDERITE M-NT 5200
- Chrome-Free Nano-Ceramic Multi-Metal Pretreatment
- Paint-Adhesion and Corrosion-Resistance Improvement
- Phosphate-Free Spray-Line Pretreatment
-
Loctite STYCAST 3103
- Low-Viscosity Solvent-Free Epoxy
- Room-Temperature or Heat Cure
- Electrically Insulating Epoxy
-
BONDERITE M-NT 5700
- Chromium-Free Ready-to-Use Aluminum Pretreatment
- Corrosion-Resistant Paint-Adhesion Conversion Layer
- Controlled Temperature-pH-Time Processing
-
-
-
LOCTITE MSC-01
- Cleaner
- Solder paste processes
- Manual and automatic operations
-
-
-
BONDERITE M-NT 7400
- Chromium-Free Conversion Treatment
- Phosphate-Free Metal Pretreatment
- Steel, Galvanized, and Aluminum Coverage
-
Loctite 9696.060NW AERO
- Metal-to-Aluminum Epoxy Bonding
- 225 to 265 deg F Cure Window
- 250 deg F Service Temperature
-
LOCTITE 5045
- Non-Slumping RTV Application
- Flexible Shock-Absorbing Silicone
- Strain-Relief Component Reinforcement
-
BONDERITE M-PT 100NC
- Chromium-Free Aluminum Seal Rinse
- Spray or Immersion Processing
- Short Spray Treatment Window
-
-
Loctite EA 9309.3NA AERO EPOXY PASTE ADHESIVE
- High Aluminum Shear and Peel Strength
- Glass-Bead Bondline Control
- Humidity and Fluid Resistance
-
LOCTITE 5240
- Light-and-Moisture Dual Cure
- Shear-Thinning Cavity Filling
- Flexible Electrically Insulating Rubber
-
BONDERITE M-PT 7100
- Dry-In-Place Metal Post-Treatment
- Short Spray or Misting Step
- Iron-Phosphate Finish Preparation
-
LOCTITE 509
- Close-Fitting Rigid Flange Sealing
- Thixotropic Migration Control
- Immediate Low-Pressure Sealing
-
ABLESTIK 281
- Non-Sag Placement Control
- 1 x 10^15 ohm-cm Volume Resistivity
- 55 to 180 deg C Service Range
-
BONDERITE M-PT 99X
- Chromium/Phosphate-Free Reactive Resin Post-Treatment
- Painted Steel/Zinc/Aluminum Corrosion Resistance
- Ambient Spray or Immersion Application
-
LOCTITE 5127
- Vertical-Surface Gasketing Control
- No-Mix Anaerobic Flange Sealing
- Manual or Automated Dispensing
-
-
ABLESTIK 931-1
- Low-Viscosity Fine-Gap Encapsulation
- Low-Exotherm One-Step Casting Cure
- 27.6 kV/mm Dielectric Strength
-
LOCTITE SI 5248
- UV/Shadow-Area Dual Cure
- Thixotropic Low-Migration Sealing
- Flexible Electrical Insulation
-
LOCTITE 5156 VRF
- Medium-Strength Anaerobic Sealing
- Immediate Low-Pressure Sealing Capability
- UV Fluorescent Formulation
-
LOCTITE C400
- Consistent Multi-Core Flux Distribution
- Improved Challenging-Surface Wetting
- Manual or Robotic Soldering
-
-
LOCTITE SI 598
- Wide-Temperature Automotive Gasketing
- High-Elongation Cured Seal
- Automotive Fluid-Resistant Gasketing
-
BONDERITE M-ZN 181 X
- Lubricant-Retaining Phosphate Layer
- Reduced Metal-on-Metal Friction
- Batch-to-Extrusion Process Coverage
-
LOCTITE 5182
- Controlled Continuous-Bead Dispensing
- Medium-Strength Flange Sealing
- Up to 0.5 mm Gasket Replacement
-
-
Loctite EA 9377
- 2,000-Cycle Thermal-Crack Resistance
- 124 MPa Compressive Strength
- 5 mil Low-Slump Moldable Shim
-
-
BONDERITE M-ZN 210
- Zinc-Phosphate Surface Preparation
- Iron and Steel Treatment
- Pre-Finish Conversion Stage
-
LOCTITE 5203
- Easy-Disassembly Flange Sealing
- Immediate Low-Test-Pressure Resistance
- Up to 0.125 mm Flange Gaps
-
-
Loctite EA 9390 AERO
- Graphite- and Glass-Composite Repair
- Hot/Wet Strength and High Shear Modulus
- BMS 8-301 Heat-Cure Qualification
-
BONDERITE M-ZN 880
- Adhesion-Promoting Surface Treatment
- Multi-Metal Spray/Immersion Pretreatment
- Pre-Phosphate Corrosion-Resistance Improvement
-
LOCTITE AA 5810A
- Non-Silicone Polyacrylate Chemistry
- Moisture-Curing Formulation
- Powertrain Fluid Resistance
-
Loctite EA 9392 AERO Epoxy Adhesive
- 1,000 psi Aluminum Lap Shear
- Thixotropic Gap-Filling Control
- 75-Minute Working Window
-
LOCTITE 5810F
- Silicone-Free Powertrain Flange Sealing
- Heavy-Body Pre-Cure Leak Testing
- Oil-Resistant Polyacrylate Gasketing
-
-
-
-
Loctite EA 9395 AERO EPOXY ADHESIVE
- 1,200 psi Lap Shear
- Thixotropic Application Control
- Ambient-Temperature Bonding Cure
-
-
-
LOCTITE 5999
- Blow-Out-Resistant Powertrain Gasketing
- Non-Corrosive Silicone Gasket Sealing
- Thixotropic Powertrain Gasket Application
-
LOCTITE ABLESTIK ABP 6389
- High-reliability QFP manufacture
- Low outgassing
- Good adhesion to BSM & Non BSM die
-
Loctite EA 956 AERO EPOXY ADHESIVE
- 1,000 psi Lap Shear
- Room-Temperature or Accelerated Heat Cure
- Low-Viscosity Adhesive Application
-
LOCTITE MR5009
- 235 to 305 mPa s Viscosity
- Red Application-Verification Layer
- Preformed Gasket Sealing and Bonding
-
LOCTITE ABLESTIK ABP 6892
- Designed for Fingerprint Sensors
- Low stress for ultra thin glass
- Low outgassing and finest filler
-
Loctite E-30CL EPOXY ADHESIVE
- Minimally Shrinking Epoxy Bondline
- Two-Part Ambient-Cure Processing
- Adhesion to Glass
-
-
LOCTITE ABLESTIK ABP 6892BA
- Designed for Fingerprint Sensors
- Low stress for ultra thin glass
- Low outgassing and filler free
-
LOCTITE SI 5050
- Less Than 3.00% VOC Content
- Approximately 1.0 Specific Gravity
- Translucent Liquid or Paste Form
-
LOCTITE ABLESTIK ABP 8035
- Heat cure
- Transparent liquid
- LED applications
-
LOCTITE SI 5901
- 20 to 50 g/min Extrusion
- 7 to 24 Minute Tack-Free
- 1 to 2 N/mm2 Zinc-Dichromate Lap Shear
-
-
LOCTITE ABLESTIK 12-1
- Thermally Conductive Bonding
- Reworkable Bonding Material
- Up to 200 deg C Service
-
LOCTITE SI 5950
- 14-Minute Shadow-Area Tack-Free
- 250 to 425 g/min Extrusion
- At Least 180% Cured Elongation
-
LOCTITE ABLESTIK ABP 8037TI
- High-reliability LED manufacture
- High thermal conductivity
- Small die on Au-finish LF
-
Loctite EA 9837.1 030OST AERO
- Long-Open-Time Composite Surfacing
- Fast 121/177 deg C Cure
- High-Adhesion Composite Surface Film
-
-
-
-
LOCTITE ABLESTIK ABP 8420
- Fast cure - Low temp also possible
- Excellent RBO performance
- Lid attach - Optical sensors & 3d modules
-
Loctite EA 9360 AERO Epoxy Adhesive
- Toughened Structural Epoxy Bonding
- 50-Minute Assembly Pot Life
- Room-Temperature Aircraft Bonding Cure
-
-
EA 9628 060NW Aero
- Toughened Structural Bonding
- Knitted or Non-Woven Nylon Carrier
- Lap-Shear, Peel, and Environmental Performance
-
-
-
ECCOBOND 334-1
- 8-Hour Work Life at 25 deg C
- Moisture Cure in About 1 to 4 Days
- One-Part Tungsten-Filled RTV
-
LOCTITE ABLESTIK DX20C
- Translucent
- Non conductive
- For GaN LEDs
-
-
-
LOCTITE 5039
- Deep Light-Cure Gasketing
- Shadow-Area Moisture Cure
- Continuous-Bead Semi-Flowable Application
-
-
LOCTITE EC210
- General-Purpose Electrical Insulation Coating
- 55:35 Two-Part Mixing
- 55 to 150 deg C Service Range
-
-
LOCTITE SI 5049
- 8 to 10 Minute Tack-Free Time
- At Least 400% Cured Elongation
- -34 to 204 deg C Temperature Exposure
-
LOCTITE ABLESTIK QMI 516IE
- Electrically conductive
- Hydrophobic
- Snap cure
-
LOCTITE SI 5075
- Self-Fusing Silicone Wrap
- -54 to 260 deg C Operating Range
- 300% Final-Material Elongation
-
-
-
-
-
-
-
LOCTITE SI 598HB
- At Least 60-Second Blow-Out Resistance
- At Most 25-Minute Tack-Free Time
- At Least 350% Cured Elongation
-
-
LOCTITE ABLESTIK QMI529HT
- Void free bondline
- Excellent thermal conductivity
- Stable at high temperatures
-
-
-
-
-
TEROSON MS 5570
- One-Component Moisture-Cure Polymer
- Fast Skin-Over Processing
- Elastic Structural Bonding
-
-
LOCTITE ABLESTIK 2111
- Thixotropic Vertical/Overhead Bonding
- 24 N/mm^2 Aluminum Lap Shear
- Glass/Metal/Plastic Substrate Compatibility
-
LOCTITE SI 595
- Non-Slumping Sealant Formulation
- Adhesion and Flexiblity
- Non-Flammable Sealing Formulation
-
LOCTITE AA 3381
- Fast 365 nm Light Fixturing
- High-Elongation Glass Joint Sealing
- Dissimilar Rigid-Substrate Bonding
-
-
ABLESTIK 342-3.5
- Two-Part Ambient-Cure Processing
- 5,000 mPa s Application Viscosity
- 29.0 N/mm^2 Aluminum Lap Shear
-
-
-
ABLESTIK 45LV
- Flexible Cured Adhesive
- 16,000 to 30,000 mPa s Mixed Viscosity
- 16 kV/mm Dielectric Strength
-
LOCTITE 3922
- Low-Viscosity Cannula Bonding
- Fast UV/Visible-Light Fixturing
- Sterilization-Tested Needle Assemblies
-
-
ABLESTIK 970-1N1
- Thixotropic Application Control
- 20.7 N/mm^2 Aluminum Lap Shear
- 90-Minute Working Window
-
-
-
-
LOCTITE 4047
- Rapid Blue-or-UV Photocure
- High-Viscosity Placement Control
- Low-Shrink Mechanical Stability
-
LOCTITE ABLESTIK QMI9507-2C2
- Controlled bondline thickness
- High thermal conductivity
- Stable at high temperatures
-
ABLESTIK FDA 2
- 1.20 x 10^14 ohm-cm Volume Resistivity
- 3-Hour Working Window
- 1,800 psi Aluminum Lap Shear
-
-
ABLESTIK FDA 22
- 1.50 x 10^14 ohm-cm Volume Resistivity
- 3-Hour Working Window
- 2,100 psi Aluminum Lap Shear
-
LOCTITE 5056
- Rapid UV Silicone Cure
- Low-Viscosity Potting and Coating
- Transparent Elastomeric Final State
-
-
ABLESTIK FDA 2T
- 1.20 x 10^14 ohm-cm Volume Resistivity
- 3-Hour Working Window
- 1,800 psi Aluminum Lap Shear
-
LOCTITE AA 326
- One-Component Activator Cure
- Controlled High-Viscosity Placement
- Ferrite-to-Metal Structural Bonding
-
ABLESTIK GA 47-2LV
- Gyro-Flotation-Fluid-Compatible Instrument Bonding
- 25 ppm/deg C Linear Thermal Expansion
- 2-Hour 95 deg C Cure
-
LOCTITE ECCOBOND EO 1061
- Extended Pot-Life Processing
- Stable-Viscosity Dispensing Control
- One-Part Heat-Cure Encapsulation
-
LOCTITE AA 3341
- Low-Viscosity Thermoplastic Bonding
- Fast UV/Visible-Light Cure
- Flexible 220% Elongation
-
ABLESTIK SF 40
- Low-Density Syntactic Foam Adhesive
- Thixotropic Vertical-Surface Control
- Room-Temperature Adhesive Cure
-
ECCOBOND FP4546
- Low-CTE Flip-Chip Underfill
- Toughened Crack-Resistant Epoxy
- 32-Hour Pot Life at 25 deg C
-
-
-
LOCTITE AA 3943
- Cannula-Focused Medium-Viscosity Dispensing
- Sub-5-Second UV Fixture
- UV-Fluorescent Assembly Inspection
-
LOCTITE 736
- Passive-Surface Cure Acceleration
- Very-Low-Viscosity Surface Wetting
- 30-Minute On-Part Activity
-
LOCTITE H8000
- Visible 10:1 Mix Confirmation
- 30-Minute Assembly Window
- Resilient Peel and Impact Performance
-
LOCTITE HY 4080
- Equal-Volume Hybrid Mixing
- 10-Minute Fixture on Metals
- Tough Peel and Impact Performance
-
LOCTITE 7380
- Solvent-Free Toughened Acrylic Activation
- Up to 6-Hour Active Window
- Fast LOCTITE 330 Fixture Development
-
LOCTITE 7451
- Pre- or Post-Activation Flexibility
- Very-Low-Viscosity Cyanoacrylate Application
- Rapid Cyanoacrylate Fixture Development
-
-
LOCTITE A-534R
- No-Drying-Time Cure Activation
- Very Low-Viscosity Application
- Fast Toughened-Acrylic Fixture Response
-
LOCTITE EA 2000
- Low-VOC Water-Based Nitrile-Phenolic Primer
- Blue-to-Blue-Green Color Change
- BMS 5-42 Type 3 Qualification
-
LOCTITE EA 9203
- No-Bake Room-Temperature Priming
- Brush-or-Spray Application Flexibility
- Adhesion Promotion on Limited-Preparation Surfaces
-
LOCTITE SF 7515
- No-Rinse Spray or Wipe
- 20 to 40 deg C Application
- Aluminum, Zinc, and Steel Pretreatment
-
-
-
-
-
LOCTITE 5055
- Low-Viscosity Medical Assembly Bonding
- Fast UV/Visible Tack-Free Cure
- Tough Transparent Silicone Rubber
-
LOCTITE SI 5091
- Self-Leveling Cavity Filling
- UV and Moisture Cure Access
- Flexible Shock-Absorbing Seal
-
LOCTITE SI 5290
- 100 to 350 mPa s Viscosity
- -53 to 204 deg C Operating Range
- 18 kV/mm Dielectric Strength
-
LOCTITE SI 5296
- 150 to 235 mPa s Viscosity
- 7-Minute Tack-Free at 125 deg C
- 20.6 kV/mm Dielectric Strength
-
-
LOCTITE SI 5056
- 1,400 to 3,000 mPa s Viscosity
- At Least 4 mm Depth in 60 Seconds
- 22.8 kV/mm Dielectric Strength
-
-
-
STYCAST 1090SI
- High Compressive-Stress Potting
- Low-Density Deep-Ocean Encapsulation
- 30-Minute Pot Life
-
STYCAST 1217
- Low-Viscosity Coil Impregnation
- Catalyst-Selectable Working Window
- Clear Inspection-Friendly Encapsulation
-
-
STYCAST 1265
- Soft-Gel Stress-Sensitive Encapsulation
- Extended 24-Hour Work Life
- Cuttable Repair Access
-
-
-
STYCAST 1266
- Low-Viscosity Fine-Gap Impregnation
- Optically Clear Encapsulation
- Flexible Ambient or Heat Cure
-
STYCAST 1495K
- Thermally Conductive Electronic Potting
- 45-Minute CAT 9 Work Life
- Transformer and Sensor Encapsulation
-
LOCTITE EA E-40HT
- Extended-Work-Life Structural Bonding
- Elevated-Temperature Epoxy Bonding
- Tough Shear- and Impact-Resistant Bondline
-
STYCAST 2057
- Low-Abrasion Meter-Mix Processing
- Machine-Dispensable Epoxy Encapsulation
- Post-Molding Machining Capability
-
-
STYCAST 2651-1
- One-Component Production Handling
- -40 to 155 deg C Service
- Thermal-Shock-Resistant Electronic Encapsulation
-
-
STYCAST 2651-40FR
- Low-Viscosity Potting Process
- Flame-Retardant Cured Encapsulation
- Low-Temperature Operating Range
-
-
LOCTITE EA 1C
- Multi-Material Metal/Plastic/Wood Bonding
- Machineable Sandable Cured Epoxy
- Low-Outgassing Epoxy Adhesive
-
ECCOBOND UV 3000
- UV-Curable Epoxy Chemistry
- High-Temperature Performance
- Low Outgassing and Chemical Resistance
-
STYCAST 2662
- High-Temperature 230 deg C Service
- Extended 24-Hour Working Window
- Staged Large-Casting Cure
-
LOCTITE 190015
- No-Mix Anaerobic Bonding
- Flexible Cured Bond Profile
- Primer-Assisted Larger-Gap Bonding
-
-
STYCAST 2741
- Catalyst-Adjusted Cured Flexibility
- Shock- and Impact-Resistant Potting
- Room-Temperature or Accelerated Cure
-
LOCTITE AA 3105
- Low-Viscosity Close-Fit Assembly
- Sub-5-Second Light Fixture
- Flexible Light-Cured Bonding
-
-
LOCTITE E-00NS
- Clear Two-Component Epoxy
- 3.5-Minute Working Life
- High-Dielectric-Strength Epoxy Adhesive
-
STYCAST 2741LV
- Lower-Viscosity Electronic Potting
- Selectable Rigid-to-Flexible Cure
- Impact-Resistant Multi-Substrate Encapsulation
-
LOCTITE AA 3201
- Rapid Light-Cure Fixture Development
- Thixotropic Placement Control
- Flexible Transparent Polycarbonate Bonding
-
LOCTITE E-04
- Two-Component Adhesive System
- Thixotropic Application Control
- Low-Shrinkage Epoxy Bonding
-
-
-
-
-
-
LOCTITE 3872
- Self-Shimming Thermal Bondline
- UV Fixture Before Heat Cure
- Low-Modulus Thermal Attachment
-
-
LOCTITE 3873
- Controlled 0.127 mm Thermal Bondline
- Thermally Conductive Permanent Attachment
- Activator-Cure Power-Device Bonding
-
LOCTITE E-60HP
- Extended 60-Minute Working Life
- Toughened Structural Epoxy Bonding
- Electrical-Insulating Cured Bondline
-
LOCTITE 3876
- Primer-Free Room-Temperature Cure
- Fast 3 to 5 Minute Fixture
- Structural Thermal Heat-Sink Bonding
-
LOCTITE EA 3981
- One-Component No-Mix Adhesive
- Heat Cure as Low as 100 deg C
- Disposable-Needle/Syringe/Lancet Cannula Bonding
-
-
LOCTITE EA 445
- Pre-Measured Two-Component Mixer Cup
- 2 to 3-Minute Gel Time
- Drillable, Tappable, Sandable Cured Epoxy
-
LOCTITE 534
- Repositionable Cut-Gasket Retention
- Direct-Contact Stick Application
- Controlled Semi-Solid Gasket Dressing
-
-
LOCTITE AA A-671
- Fast Room-Temperature Fixture
- High-Strength Magnet Bonding
- External-Mix 1:1 Processing
-
LOCTITE AA 3108
- Fast UV-Cure Potting
- High-Elongation Cured Protection
- Dielectric Encapsulation Performance
-
LOCTITE EA 901NA-B1
- Thixotropic Gap-Filling Control
- 50-Minute Working Window
- Room-Temperature Application Cure
-
LOCTITE AA 331
- Rapid Activator-Assisted Fixture
- High-Strength Metal Bonding
- Magnet Assembly Impact Resistance
-
LOCTITE AA 332
- High-Viscosity Magnet Bonding
- Fast Activator-Assisted Fixture
- Impact- and Peel-Resistant Bonds
-
LOCTITE EA 9309.2
- 40 lb/in Peel Strength
- 37.2 MPa Aluminum Lap Shear
- Moderate-Viscosity Two-Part Paste
-
LOCTITE EA 9309.3
- Glass-Bead Bondline Control
- 34.5 MPa Aluminum Lap Shear
- Lap Shear Was Evaluated After hot/wet
-
-
LOCTITE EA 9309NA
- High Peel Strength on Prepared Aluminum
- Glass, Metal, and Wood Bonding
- 1-Hour 180 deg F Cure
-
-
-
LOCTITE AA 3963
- Fast Tack-Free LED Cure
- Low-Viscosity Rigid Bonding
- Strong Polycarbonate Assembly Bonds
-
-
LOCTITE AA 3971
- Post-Assembly Needle-Well Dispensing
- Dual-Wavelength Five-Second Fixture
- Black-Light Assembly Inspection
-
LOCTITE EA 9330
- High Aluminum Peel and Lap-Shear Strength
- 60-Minute Working Window
- Multi-Fluid and Salt-Spray Resistance
-
-
-
-
LOCTITE AA H8500
- Spacer-Bead Bondline Control
- 25-Minute Steel Assembly Window
- High-Impact Steel Bonding
-
-
LOCTITE AA H8600
- Non-Sag Vertical Application
- 25-Minute Open Working Window
- Galvanized-Steel Peel and Impact
-
LOCTITE EA 9394.3
- 4,200 psi Aluminum Lap Shear
- 90-Minute Working Window
- Thixotropic Gap-Filling Control
-
LOCTITE EA 9394C-2
- 1-Hour 204 deg C Cure
- Extended Working Window for Controlled Assembly Operations
- Qualified to MMM-A-132 Type Ii
-
LOCTITE AA 3462
- Rapid UV/Visible Light Cure
- Flexible Shock-Absorbing Bondline
- Glass Bonding Across Multiple Materials
-
LOCTITE AA 3921
- 5-Second UV/Visible-Light Cure
- Transparent Cured Bondline
- High-Hardness Acrylic Adhesive
-
LOCTITE EA 9394S
- 28.9 MPa Aluminum Lap Shear
- Controlled Two-Part Processing
- Paste-Form Adhesive Application
-
LOCTITE EA 9396.6MD
- Two-Part Potting/Edge-Fill Syntactic Epoxy
- Controlled Processing Window
- Elevated-Temperature Mechanical Properties
-
LOCTITE AA 3922
- Second-Scale UV Fixture
- Low-Viscosity Precision Bonding
- UV-Fluorescent Bond Inspection
-
-
LOCTITE DSP 190024
- Fast UV Fixture Development
- Thixotropic Edgebond Placement
- No-Post-Cure Electronics Bonding
-
-
LOCTITE H5004
- Fast Room-Temperature Fixture
- Clear High-Peel Structural Bonds
- 1:1 Static-Mix Processing
-
LOCTITE EA 9460
- Impact/Fatigue-Resistant Cured Epoxy
- 40 to 65-Minute Pot Life
- Multi-Material Metal/Thermoplastic/Laminate Bonding
-
ECCOBOND EO 1080
- 20-Minute Cure at 150 deg C
- 12-Month Shelf Life at 4 deg C
- 177 deg C Continuous Service
-
LOCTITE EA 960F
- Aircraft Fairing and Smoothing
- Controlled Rapid Processing
- Documented Aluminum Bond Performance
-
-
LOCTITE EA 9696
- High-Toughness Aerospace Bonding
- Broad Controlled Cure Window
- 2,000-Hour Environmental Conditioning
-
STYCAST US 0138
- Extended 40-to-60-Minute Working Time
- Ambient or Accelerated Cure
- Electrically Insulating Electronic Potting
-
STYCAST US 1150
- Convenient 1:4 Meter-Mix Ratio
- Extended 60-Minute Working Time
- Low-Temperature Hardness Stability
-
LOCTITE EA E-60NC
- Flowable Electronic Potting
- Extended 60-Minute Working Window
- Electrical Insulation After Cure
-
-
LOCTITE EA E-120HP
- 120-Minute Working Life
- Peel, Impact, Thermal-Shock, and Chemical Resistance
- Aerospace and Industrial Bonding
-
-
LOCTITE ECCOBOND 50300-1
- One component
- Low CTE
- Low viscosity
-
LOCTITE EA E-20NS
- Non-Sag Vertical Bonding
- Tough High-Peel/Shear Bonding
- Electrically Insulating Multi-Material Bonding
-
-
LOCTITE EA E214HP
- One-Component, No-Mix Epoxy Paste Simplifies Material Preparation
- 37 N/mm^2 Stainless-Steel Lap Shear
- 22 kV/mm Dielectric Strength
-
LOCTITE ECCOBOND 50300LT
- High wire profile
- Less thixotropic
- Glob top
-
-
-
LOCTITE EA M-121HP
- Non-Sag Placement Control
- Two-Part, Room-Temperature-Curing System
- Prepared Metals Bonding
-
-
-
-
-
LOCTITE EA 9306NA
- One-Component, Heat-Curing Epoxy Paste
- Low-Exotherm Bonding Processing
- 34.5 MPa Aluminum Lap Shear
-
-
LOCTITE EA 9394
- Two-Part Aerospace Structural Epoxy Paste
- 177 deg C Service Temperature
- MMM-A-132 Qualified Epoxy
-
LOCTITE ECCOBOND CB064
- High purity
- Very low CTE (7 ppm/°C)
- Also known as FP4653
-
LOCTITE HY 4090
- Cyanoacrylate/Epoxy Hybrid Adhesive
- Below 180-Second Fixture Time
- Steel/Aluminum/Polycarbonate Lap-Shear Bonding
-
-
LOCTITE M-21HP
- Two-Component Adhesive System
- High Peel Resistance
- Room-Temperature Curing Epoxy Bonding
-
-
-
-
-
-
-
-
LOCTITE ECCOBOND FP4450
- Fill Encapsulant
- High purity
- Good moisture resistance
-
-
LOCTITE ECCOBOND FP4451
- Encapsulant - DAM
- High purity
- Minimal slumping
-
-
-
-
-
-
LOCTITE ECCOBOND FP4654
- High purity
- Self levelling
- Low stress
-
-
-
LOCTITE ECCOBOND ME995-1-4
- One component
- Thermally conductive
- High viscosity
-
LOCTITE ECCOBOND UV8800M
- UV Cure
- Cures rapidly
- Excellent adhesion
-
LOCTITE ECCOBOND UV8800M-X
- Fast UV Cure
- Good workability
- Good adhesion
-
-
-
-
-
-
-
-
-
-
-
-
STYCAST US 5529
- Low-Viscosity Potting Flow
- Extended 45-Minute Working Time
- Flexible Cured Polyurethane
-
-
LOCTITE STYCAST PC18M
- Conformal Coating
- For environmental and moisture protection
- Room temperature cure
-
-
-
-
LOCTITE SI 5611F
- Self-Leveling Electronic Encapsulation
- Fast Tack-Free Cure Profile
- High-Resistivity Silicone Insulation
-
LOCTITE E-60NC
- Two-Component Adhesive System
- Low-Viscosity Adhesive Application
- Non-Corrosive Bonding Formulation
-
LOCTITE EA 11C
- Machinable, Low-Outgassing Cured Material
- Bonds Metals, Most Plastics and Wood
- Room-Temperature or Heat Cure
-
-
LOCTITE EA 9807
- Pourable Intermediate-Density Epoxy Syntactic
- Room-Temperature or Heat Cure
- 121 deg C Service Temperature
-
LOCTITE EA 9825
- Low-Density, One-Component Epoxy Syntactic
- Up to 350 deg F Service
- Honeycomb Composite Potting
-
-
LOCTITE ES6010
- Low-Viscosity Electronics Potting
- 80-to-100-Minute Working Time
- Room-Temperature or Heat Cure
-
LOCTITE EA 3943
- Cannula-Focused Medium-Viscosity Dispensing
- Sub-5-Second UV Fixture
- UV-Fluorescent Assembly Inspection
-
LOCTITE SI 5210
- Ultra-Fast RTV Silicone Cure
- Non-Corrosive Alkoxy-Cure Potting
- Thixotropic Non-Sag Application
-
LOCTITE EA 460
- Low-Odor Low-Bloom Bonding
- Low-Viscosity Precision Application
- Rapid Multi-Substrate Fixture
-
LOCTITE SI 5640
- Low-Viscosity Self-Leveling Potting
- Off-White Part A and Black Part B
- 490 mL Two-Part Cartridge
-
LOCTITE EA 7000
- Dual-Temperature Composite Cure
- Extended 30-Day Out Time
- Supported or Unsupported Film
-
LOCTITE EA 9017
- Premeasured Resin-Hardener Pack
- Fast 4-6-Minute Handling
- Machinable Cured Epoxy Finish
-
LOCTITE EA 9340
- Visual 1:1 Mix Confirmation
- Extended 90-Minute Pot Life
- High-Temperature Shear Retention
-
-
-
LOCTITE EA 9658.060UNS
- Unsupported 0.060 lb/sf Film
- 177 deg C Cure Capability
- Extended 15-Day Assembly Window
-
LOCTITE EA 9658.100
- Non-Woven Glass Film Support
- 177 deg C High-Temperature Cure
- Extended 15-Day Assembly Window
-
LOCTITE EA 9686.060
- Tough Aerospace Structural Bonding
- Tough Elevated-Temperature Bonding
- Metal Composite Honeycomb Assembly
-
-
-
LOCTITE EA 9814
- One-Part Syntactic Processing
- Low-Density Honeycomb Core Filling
- Fire-Retardant Compressive Support
-
LOCTITE EA 9845SF
- Co-Cured Composite Surfacing
- Paint-Ready Surface Quality
- Reduced Core Crush and Porosity
-
LOCTITE EA 9845SF.030OST
- Controlled .030 OST Surface Layer
- Co-Cure Composite Integration
- Paint-Ready Composite Finish
-
LOCTITE EA 9891RP
- Visual Color-Change Mix Verification
- Room-Temperature Abradable Seal Repair
- Abrasion-Resistant Paste Restoration
-
LOCTITE EA 9895
- One-Piece Peel-Ply Removal
- Bond-Ready Surface Without Sanding
- 177 deg C Prepreg Co-Cure
-
LOCTITE EA E-40EXP
- Self-Leveling Horizontal Potting
- Controlled 2:1 Metered Mixing
- Room-Temperature Potting Cure
-
LOCTITE EA9690.030NW
- High-Peel Structural Bonding
- Low-Flow Film Placement
- Thin Non-Woven Film Handling
-
LOCTITE EF557
- Expanding Honeycomb Gap Filling
- Film-Based Splice Reinforcement
- Dual-Temperature Cure Flexibility
-
LOCTITE EF562S
- Non-Asbestos Honeycomb Bonding
- Roll-or-Sheet Layup Flexibility
- Expanding Core Reinforcement
-
STYCAST 2760
- Vinyl-Wire Potting Adhesion
- 60-Minute Low-Viscosity Processing
- Room-Temperature or Heat Cure
-
-
-
ABLESTIK A359
- Up To 200 deg C Intermittent Use
- 3-Minute 175 deg C Cure
- 17.2 N/mm^2 Steel Shear Strength
-
ECCOBOND SF40
- 0.64 g/cm^3 Mixed Density
- 30-Minute Work Life
- Up to 14.5 MPa Aluminum Lap Shear at 25 deg C
-
LOCTITE 3129
- Low-Temperature 80 deg C Cure
- Extended 21-Day Pot Life
- Heat-Sensitive Electronics Bonding
-
-
-
LOCTITE EA 3471
- Machinable Metal-Like Repair Finish
- Non-Sag Rebuilding Putty
- Room-Temperature Metal Repair
-
-
-
LOCTITE EA 7363
- Non-Sag Anchor-Hole Application
- 20-Minute Anchor Placement Window
- Seismic Anchoring and Grouting
-
LOCTITE EA 9035
- Rapid Four-Minute Repair Window
- Non-Sag Vertical Placement
- Equal-Part 1:1 Cartridge Mixing
-
LOCTITE EA 9361
- High-Elongation Flexible Bonding
- Long 120-Minute Pot Life
- Cryogenic Lap-Shear Performance
-
LOCTITE EA 9380
- Low-Temperature Heat-Cure Bonding
- Extended Three-Hour Assembly Window
- High-Strength Toughened Paste Bonding
-
LOCTITE EA 9380.05
- Long Two-to-Three-Hour Assembly Window
- Meter-Mix Large-Part Application
- Low-Temperature 82 deg C Cure
-
LOCTITE EA 9499.4
- Single-Component Paste Handling
- Heat-Cure Expanding Fill
- Aerospace Syntactic Gap Filling
-
LOCTITE EA 9695 .030 PSF NW
- Low-Flow Prepreg Resin Control
- Extended Open Assembly Window
- Composite Co-Cure and Repair
-
LOCTITE EA 9695 .050 PSF
- Low-Flow Composite Co-Cure
- Dual-Temperature Heat Cure
- Composite Laminate Bonding and Repair
-
LOCTITE EA 9820
- Extended >8-Hour Work Life
- Low-Flow Honeycomb Potting
- High Compressive Strength Syntactic Fill
-
LOCTITE EA 9824 FST
- FST-Compliant Formulation
- Low-Density Epoxy System
- Automated Dispensing Capability
-
LOCTITE EA 9845LC
- Conductive Copper-Foil Lightning Surfacing
- Honeycomb Surface-Leveling Control
- Micro-Crack and UV Resistance
-
LOCTITE EA E-04SS
- Very-Fast Cure for Short Cycles
- Mixed-On-Demand Two-Part System
- Metal Seam-Sealing Application
-
LOCTITE EA E-05CL
- Fast 3-Minute Working Window
- Ultra-Clear Flexible Bonding
- Electrically Insulating Cured Epoxy
-
LOCTITE EA E-05MR
- Matched 1:1 Volume or Weight Mixing
- Fast 10 to 15 Minute Fixture
- Ultra-Clear Impact-Resistant Bonding
-
LOCTITE EA E-1962
- No-Mix One-Part Processing
- Heat-Cure Precision Bonding
- Stainless-Steel, Glass, and Plastic Bonding
-
LOCTITE EA E-40FL
- Flexible Dissimilar-Material Bonding
- 40-Minute Working Window
- Shock- and Impact-Resistant Bondline
-
LOCTITE EA 3985
- Fast Heat-Cure Production Bonding
- Non-Sag Wire-to-Armature Application
- One-Part No-Mix Processing
-
-
-
-
-
LOCTITE PE 3140
- 11,000 cP Resin Viscosity
- 3.1:1 PE 3160 Volume Mixing
- 80 to 100 Minute PE 3160 Work Time