BONDERITE S-ST 6776-LO
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Vertical and Overhead Surface Cling
- Ready-to-Use Spray or Manual Application
- Epoxy and Polyurethane Paint Removal
Product Description
BONDERITE S-ST 6776 LO AERO is a one-part, low-odor thixotropic paint stripper for removing epoxy, polyurethane, and other catalyzed coatings from approved aerospace metal substrates. The viscous green liquid is supplied ready to use and is designed to cling to vertical and overhead surfaces during spray or manual application. It can be used on aluminum, mild steel, cast iron, and titanium, while high-strength steel and magnesium are excluded from the documented substrate scope. Its chemistry contains no methylene chloride, chlorinated solvents, phenols, chromates, ammonia, or amines, supporting a differentiated stripping option for controlled aerospace maintenance processes.
Key features
- Vertical and Overhead Cling: The thixotropic liquid is designed to remain on vertical and overhead surfaces.
- Ready-to-Use Application: Supplied for spray or manual use without required mixing or dilution.
- Catalyzed-Coating Removal: Removes epoxy, polyurethane, and other catalyzed paint systems from listed aerospace metals.
Applications
Removal of epoxy, polyurethane, and catalyzed paint systems from approved aluminum, mild steel, cast iron, and titanium surfaces by spray or manual application.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Viscous green liquid | As supplied | |
| Brookfield viscosity | Greater than 15,000 | mPa s | 20 deg C; 6 rpm |
| pH | 2.5 to 3.0 | As supplied | |
| Optimal storage temperature | 5 to 35 | deg C | Storage condition |