BONDERITE M-FE 330SW
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Three-Function Aluminum Pretreatment
- Defined 60 to 120 deg F Window
- Explicit High-Copper Alloy Exclusion
Product Description
BONDERITE M-FE 330SW is a phosphoric-acid, surfactant-based metal-pretreatment fluid for cleaning, brightening, and conditioning aluminum surfaces. It prepares a chemically clean, soil-free surface before welding, painting, or coating and can be applied by steam gun or high-pressure manual methods. The product operates within a 60 to 120 deg F temperature range and a 7.5 to 37.5-point total-acid range. It is not recommended for high copper-bearing aluminum alloys or aluminum castings, a boundary that should remain part of product selection.
Key features
- Three-in-One Aluminum Treatment: Cleans, brightens, and conditions aluminum surfaces before subsequent finishing.
- Defined Operating Window: Uses a 60 to 120 deg F temperature range and 7.5 to 37.5-point total-acid range.
- Clear Alloy Boundary: Not recommended for high copper-bearing aluminum alloys or aluminum castings.
Applications
Cleaning, brightening, and conditioning aluminum before welding, painting, or coating by steam gun or high-pressure manual application.