LOCTITE IS 5110
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated
Main features
- Low-Viscosity Leak-Path Impregnation
- Water-Rinsable Post-Impregnation Cleanup
- Anaerobic Sealing Inside Porosity
Product Description
LOCTITE IS 5110 is a one-component, low-viscosity anaerobic sealant for vacuum impregnation of interfacial leak paths in rigid electronic assemblies. Its typical viscosity is 36 to 66 mPa s at 25 deg C, allowing liquid sealant to saturate internal porosity during vacuum impregnation. Excess material disperses in water and is rinsed from exterior surfaces before the retained sealant cures in the absence of freely available oxygen. The cured thermoset has Shore D 89 hardness, volume resistivity of 9 x 10^13 ohm cm, and a continuous-temperature design limit of 205 deg C. Applications include overmolded components, connectors, coils, lamination stacks, solenoids, and sealed enclosures.
Key features
- Low-Viscosity Vacuum Impregnation: Typical viscosity is 36 to 66 mPa s at 25 deg C for the vacuum-impregnation process.
- Water-Dispersible Excess Sealant: Excess liquid disperses in water for post-impregnation rinsing from exterior surfaces.
- Anaerobic Internal Cure: Sealant retained inside porosity polymerizes where freely available oxygen is absent.
Applications
Vacuum impregnation and leak-path sealing in overmolded electrical components, connectors, high-temperature coils, lamination stacks, solenoids, and sealed enclosures.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.09 | - | Typical; 25 deg C |
| Surface tension | 42.3 | dynes/cm | Typical; ASTM D1590 |
| Viscosity | 36 to 66 | mPa s | LMS range; Brookfield RVT, 25 deg C, spindle 2, 50 rpm |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shore hardness | 89 | Durometer D | Typical; ISO 868 |
| Continuous-temperature design limit | 205 | deg C | Design limit; continuous temperature |
| Compressive modulus | 1,790 | N/mm^2 | Typical; ISO 604 |
| Flexural modulus | 1,740 | N/mm^2 | Typical; ASTM D790 |
| Volume resistivity | 9 x 10^13 | ohm cm | Typical; IEC 60093 |
| Dielectric breakdown strength | 39.4 | kV/mm | Typical; IEC 60243-1 |