LOCTITE PE3164

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

LOCTITE PE3164

Main features

  • 105 cP Hardener Viscosity
  • 2:1 PE 3140 Volume Mixing
  • 10 to 15 Minute System Work Time

Product Description

LOCTITE PE 3164 is the clear epoxy hardener component used as Part B with LOCTITE PE 3140 resin in a two-part potting system. As supplied, PE 3164 has 105 cP viscosity at 25 deg C using spindle 2 at 20 rpm and a specific gravity of 0.97. The PE 3140 and PE 3164 system mixes at 2:1 resin-to-hardener by volume and has a 10 to 15 minute work time for a 400 g mass at 25 deg C. Cure time is 16 hours at 25 deg C or 2 hours at 66 deg C.

Key features

  • 105 cP Hardener Viscosity: PE 3164 hardener viscosity is 105 cP at 25 deg C using spindle 2 at 20 rpm.
  • 2:1 PE 3140 Volume Mixing: The PE 3140 and PE 3164 system uses a 2:1 resin-to-hardener ratio by volume.
  • Paired-System Working Time: The PE 3140 and PE 3164 system has a 10 to 15 minute work time for a 400 g mass at 25 deg C.

Applications

Hardener component for the LOCTITE PE 3140 two-part potting system.

Product Family

LOCTITE PE3164

Loading pricing…

Technical Specifications

General Properties
Color
The color
Clear
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.96
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
450 mPa.s

Additional Information

Technical properties

As supplied

Values apply to the LOCTITE PE 3164 hardener component only.

PropertyValueUnitMethod / condition
AppearanceClearPE 3164 hardener, as supplied
Viscosity105cPPE 3164 hardener; spindle 2, 20 rpm, 25 deg C
Specific gravity0.97PE 3164 hardener, as supplied
Storage temperature8 to 28deg CUnopened container unless otherwise labeled