ECCOBOND UV 3000

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

ECCOBOND UV3000

Main features

  • UV-Curable Epoxy Chemistry
  • High-Temperature Performance
  • Low Outgassing and Chemical Resistance

Product Description

LOCTITE ECCOBOND UV 3000 is a clear, UV-curable epoxy adhesive designed for high-throughput assembly operations. The material cures through ultraviolet light using a cationic cure mechanism and is commonly used for glass bonding and optoelectronic lens attachment applications. With a medium viscosity of approximately 5,300 cP, low outgassing characteristics, chemical resistance, and thermal stability at temperatures up to 200°C, it can support demanding bonding applications where optical clarity, environmental resistance, and elevated-temperature performance are important considerations.

Key features

  • UV-curable epoxy chemistry: Supports rapid processing using UV exposure for high-throughput manufacturing environments.
  • High-temperature performance: Can withstand exposure to temperatures as high as 200°C.
  • Low outgassing and chemical resistance: Suitable for applications where contamination control and environmental durability are important.

Applications / Suitable for

  • Glass bonding
  • Lens attachment
  • Optoelectronic assemblies
Product Family

ECCOBOND UV 3000

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear
Specific Gravity
1.09
Physical Properties
Viscosity
5,300 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
150 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties and handling information.

Property Value Unit Method / condition
Appearance Clear — As supplied
Viscosity 5,300 mPa·s (cP) Brookfield HBT, Spindle 7, 10 rpm, 25°C
Specific Gravity 1.09 — 25°C
Shelf Life 365 days From date of manufacture
Recommended UV Intensity 200 mW/cm² UV curing guideline
Technical properties

After-processing / final-state properties

Typical properties after UV cure.

Property Value Unit Method / condition
Glass Transition Temperature (Tg) 150 °C Cured material
Coefficient of Thermal Expansion (Alpha 1) 75 ppm 40–120°C
Chloride Ion Content <10 ppm 121°C extraction
Sodium Ion Content <5 ppm 121°C extraction
Potassium Ion Content <5 ppm 121°C extraction