LOCTITE 5770
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- High-Temperature Steam Thread Sealing
- High-Pressure Steel Joint Sealing
- Medium-Strength Anaerobic Locking
Product Description
LOCTITE 5770 is a high-temperature, medium-strength anaerobic dimethacrylate sealant for metal threaded pipes and fittings in industrial service. Its high-viscosity thixotropic paste is particularly suited to steel joints requiring both high-temperature and high-pressure resistance. At 25 deg C, typical specific gravity is 1.27 and typical cone-and-plate viscosity is 30,000 to 90,000 mPa s at 50 s^-1. Typical removal torque after 72 hours at 22 deg C is 74 N m on 3/8 in malleable iron tees and steel plugs pre-torqued to 27 N m. The product also sealed 100 psi air after a 5-minute cure in an ASTM D6396 fitting test and has been tested for steam resistance at temperatures up to 280 deg C.
Key features
- High-temperature steel sealing: Designed for steel threaded joints where high-temperature and high-pressure resistance is required.
- Early-cure pressure sealability: 3/8 in NPT malleable iron tees and steel plugs sealed 100 psi air after 5 minutes of cure at 22 deg C in an ASTM D6396 test.
- High-temperature steam testing: Forged-steel NPT steam assemblies were tested at temperatures up to 280 deg C and pressures up to 6.4 MPa.
Applications
Sealing metal threaded pipes and fittings, including industrial steam service.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Off-white to purplish gray paste | - | Uncured |
| Specific gravity | 1.27 | - | Typical; 25 deg C |
| Viscosity | 30,000 to 90,000 | mPa s | Typical; cone and plate; 25 deg C; 50 mm parallel plates; 0.5 mm gap; 50 s^-1 |
Cured properties and performance
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Breakloose torque | 9.0 to 28.4 | N m | Typical; ISO 10964; after 24 h at 25 deg C; 3/8 x 16 grade 5 steel nuts and bolts; degreased; pre-torqued to 5 N m |
| Removal torque | 74 | N m | Typical; ASTM D6396; after 72 h at 22 deg C; 3/8 in malleable iron tees and steel plugs; pre-torqued to 27 N m |
| Air pressure sealability | 100 | psi | ASTM D6396; 3/8 in NPT malleable iron tees and steel plugs; pre-torqued to 27 N m; cured 5 min at 22 deg C |
| Steam weight loss | 0 | % | ASTM D6396-based steam test; 232 deg C; 2.9 MPa; 48 h; cured 24 h at 22 deg C plus 2 h at 150 deg C |
| Steam weight loss | 4 | % | ASTM D6396-based steam test; 280 deg C; 6.4 MPa; 48 h; cured 24 h at 22 deg C plus 2 h at 150 deg C |