LOCTITE LB 8423

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8423

Main features

  • 19.8 kV/mm Dielectric Strength
  • 2.6 x 10^15 ohm cm Resistivity
  • -55 to 204 deg C Operating Range

Product Description

LOCTITE LB 8423 is a non-curing silicone dielectric compound supplied as a translucent thick paste for electrical connectors and lubricated interfaces. It is used on spark plug boots, distributor cap nipples, battery terminals, ignition-coil connectors, trailer electrical connectors, and on rubber, plastic, and ceramic surfaces. Typical application operating range is -55 to 204 deg C. Electrical properties include 19.8 kV/mm dielectric breakdown strength by IEC 60243-1, dielectric constant 3.0 with dissipation factor 0.007 at 1 kHz by IEC 60250, and volume resistivity of 2.6 x 10^15 ohm cm by IEC 60093.

Key features

  • 19.8 kV/mm Dielectric Strength: Dielectric breakdown strength measured by IEC 60243-1.
  • 2.6 x 10^15 ohm cm Resistivity: Volume resistivity measured by IEC 60093.
  • -55 to 204 deg C Range: Typical application operating range is -55 to 204 deg C.

Applications

Spark plug boots, distributor cap nipples, battery terminals, ignition-coil connectors, trailer electrical connectors, and lubricated rubber, plastic, or ceramic interfaces.

Technical Specifications

General Properties
Appearance
Translucent paste
Chemistry Type
Silicone dielectric compound
Specific Gravity
1.03
Other Properties
Storage Temperature
8 °C to 21 °C
Electrical Properties
Volume Resistivity
2.6 x 10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
AppearanceTranslucent pasteAs supplied
Specific gravity1.0325 deg C
Penetration2501/10 mmISO 2137
Technical properties

In service

Non-curing grease; electrical values are bulk-compound measurements.

PropertyValueUnitMethod / condition
Operating range-55 to 204deg CTypical application range
Dielectric breakdown strength19.8kV/mmIEC 60243-1
Dielectric constant3.0IEC 60250, 1 kHz
Dissipation factor0.007IEC 60250, 1 kHz
Volume resistivity2.6 x 10^15ohm cmIEC 60093