Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 5970C

Main features

  • 40 to 80 g/min Extrusion
  • 20-Minute Skin Formation
  • At Least 200% Cured Elongation

Product Description

LOCTITE SI 5970C is a one-component black alkoxy RTV silicone gasketing compound for stamped sheet-metal covers, including timing covers and oil sumps. The thixotropic material requires no mixing and has typical Semco-cartridge extrusion of 40 to 80 g/min at 25 deg C under the stated test. It forms a skin within 20 minutes at 23+/-2 deg C and 50+/-5% RH. Typical cured properties include Shore A hardness 44, at least 200% elongation, and at least 1.5 N/mm2 tensile strength.

Key features

  • Controlled Extrusion: Typical Semco-cartridge extrusion is 40 to 80 g/min at 0.62 MPa for 15 seconds at 25 deg C.
  • Surface Skin Formation: Forms a skin within 20 minutes at 23+/-2 deg C and 50+/-5% RH.
  • Cured Flexibility: Elongation is at least 200% by ISO 37.

Applications

Gasketing; sealing.

Product Family

LOCTITE SI 5970C

Loading pricing…

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.38 - 1.44
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
200 %