LOCTITE 190828

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

LOCTITE 190828

Main features

  • Rapid Humidity-Cure Bonding
  • Thermal-Cycling-Resistant Cyanoacrylate Adhesion
  • Multi-Substrate Instant Assembly

Product Description

LOCTITE 190828 is a one-part clear cyanoacrylate instant adhesive that cures with humidity. The uncured liquid has a typical viscosity of 613 mPa s at 25 deg C, measured with a Brookfield LVF viscometer using spindle 2 at 30 rpm. It develops high handling strength rapidly after bonding and is formulated for thermal-cycling resistance. A 365-day shelf life applies when stored at 2 to 8 deg C in the unopened container. Applications include rapid bonding of metals, plastics, and elastomers.

Key features

  • Brookfield viscosity: Typical viscosity is 613 mPa s at 25 deg C.
  • Rapid humidity cure: The adhesive develops high handling strength rapidly after bonding.
  • Thermal-cycling resistance: The cyanoacrylate is formulated for thermal-cycling resistance.

Applications

Applications include rapid bonding of metals, plastics, and elastomers.

Product Family

LOCTITE 190828

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear liquid
Physical Properties
Viscosity
613 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear liquid-As supplied
Viscosity613mPa sTypical; 25 deg C; Brookfield LVF, spindle 2, 30 rpm
Shelf life365daysUnopened container; 2 to 8 deg C
Optimal storage2 to 8deg CUnopened container in a dry location