LOCTITE MR 5922

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE MR5922

Main features

  • 500,000 to 700,000 mPa s Viscosity
  • 24-Hour Full Cure
  • Preformed Gasket Repair

Product Description

LOCTITE MR 5922 is a one-part, slow-drying solvent-based gasket sealant paste for flanges, fittings, connections, flexible assemblies, and dressing or repairing preformed gaskets. It cures by solvent evaporation. Typical as-supplied properties include specific gravity 1.5 at 25 deg C, Brookfield viscosity of 500,000 to 700,000 mPa s at 25 deg C, and approximately 87% solids by weight. The slower-drying formula increases work time. After application, the assembly is operational after 4 hours, and full cure occurs after 24 hours.

Key features

  • 500,000 to 700,000 mPa s Viscosity: Brookfield RVT viscosity at 25 deg C, spindle 7, 5 rpm.
  • Cure Completion: Full cure occurs after 24 hours.
  • Preformed Gasket Repair: The sealant dresses or repairs damaged pre-cut gaskets.

Applications

Sealing flanges, fittings, connections, flexible assemblies, and dressing or repairing preformed gaskets.

Technical Specifications

General Properties
Appearance
Brown / Black viscous paste
Chemistry Type
Resin / Isopropanol / Fillers
Solids
~87 %
Specific Gravity
1.5
Physical Properties
Viscosity
500,000 to 700,000 mPa.s
Other Properties
Storage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Specific gravity1.5Typical; 25 deg C
Viscosity500,000 to 700,000mPa sTypical; Brookfield RVT, 25 deg C, spindle 7, 5 rpm
Solids contentApproximately 87% by weightTypical

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers