BONDERITE M-AD40

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE M-AD40

Main features

  • Strongly Alkaline Pretreatment Cleaning
  • Complete Water Solubility
  • Defined Low-Temperature Storage Boundary

Product Description

BONDERITE M-AD 40 is a strongly alkaline, water-based pretreatment additive and cleaner supplied as a colorless, odorless liquid. The product has a pH of 14, a specific-gravity range of 1.21 to 1.23 at 15.56 deg C, and complete solubility in water. Its defined liquid properties support controlled identification and handling within industrial pretreatment operations. Storage above 4.4 deg C protects the as-supplied product from low-temperature conditions while maintaining the documented handling boundary in use.

Key features

  • Strongly Alkaline Cleaner: The as-supplied liquid has a documented pH of 14.
  • Complete Water Solubility: The water-based product is completely soluble in water.
  • Defined Storage Minimum: Store above 4.4 deg C to avoid low-temperature exposure.
Product Family

BONDERITE M-AD40

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
>100 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.21 - 1.23

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
Physical stateLiquid-As supplied
ColorColorless-As supplied
OdorOdorless-As supplied
pH14-As supplied
Specific gravity1.21 to 1.23-At 15.56 deg C
Water solubilityComplete-As supplied
VOC content0%As supplied

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers