FREKOTE R-180

Main features

  • High-Slip Rubber Release
  • Virtually No Mold Residue
  • 4-Minute Full Cure at 150 deg C

Product Description

LOCTITE FREKOTE R-180 is a one-part, water-based, high-slip mold release emulsion for difficult-to-release rubbers and highly abrasive compounds. It is designed for spray-gun application and produces a satin-matte finish with virtually no residue in the mold. The coating cures on a heated mold without dry time between coats, and the top coat can reach full cure in four minutes at 150 deg C. Its release profile combines high slip with low mold build-up for demanding rubber-molding processes.

Key features

  • High-Slip Rubber Release: The product is designed for difficult-to-release rubbers and highly abrasive compounds.
  • Virtually No Mold Residue: The satin-matte finish leaves virtually no residue in the mold.
  • 4-Minute Full Cure at 150 deg C: The heated-mold top coat reaches full cure under the stated condition without dry time between coats.

Applications

Release of difficult rubbers; release of highly abrasive molding compounds; heated-mold release processes.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White emulsion
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.98 to 1.02
Other Properties
Storage Temperature
8°C to 21 °C