LOCTITE DRI 513HV
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- High-Temperature Thread Sealing
- Re-Adjustable Threaded Assemblies
- Dry-Film Non-Curing Seal
Product Description
LOCTITE DRI 513HV is a one-part acrylic thread sealant that dries to a resilient, tight-clinging, non-curing seal on tapered or straight threaded plastic and metal pipes and fittings. It is designed for sealing and locking threaded assemblies that may require re-adjustment after installation. Typical use temperature is -20 to 150 deg C, with intermittent exposure up to 177 deg C. The high-viscosity liquid dries to a seal for threaded fittings, sensors, connectors and related assemblies where leak resistance and adjustability are important.
Key features
- Non-curing thread seal: Dries to a resilient, tight-clinging seal on tapered or straight threads.
- Thread-Seal Temperature Range: Typical use range is -20 to 150 deg C, with intermittent exposure up to 177 deg C.
- Re-adjustable assemblies: Designed for threaded fittings where sealing and later re-adjustment are required.
Applications
Sealing and locking tapered or straight threaded plastic and metal pipes and fittings, including re-adjustment applications and common threaded fittings, sensors and connectors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.02 to 1.18 | 25 deg C; LMS | |
| Viscosity | 16,200 to 44,000 | mPa s | Brookfield RVT; spindle 6; 10 rpm; 25 deg C; LMS |
| pH | 7.0 to 8.0 | 25 deg C; LMS | |
| Solids content | 54 to 72 | % | LMS |
| On-part life | 4 | years | Stored in a cool, dry area |
Final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Typical operating temperature | -20 to 150 | deg C | Documented typical use range |
| Intermittent temperature | Up to 177 | deg C | Documented intermittent exposure |
| Heat-aged sealing | Passed 1,035 | kPa | 3/8 in malleable iron NPT; 1 min leak test after documented heat aging |
| Automotive-fluid sealing | No leakage | 12.7 mm malleable iron NPT; 30-day immersion in listed automotive fluids; 1,035 kPa for 1 min |