BONDERITE M-AD 131

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

BONDERITE M-AD 131

Main features

  • Zinc-Phosphate Bath Acceleration
  • Near-Neutral pH Profile
  • Odorless Liquid Process Additive

Product Description

BONDERITE M-AD 131 is a liquid zinc-phosphate accelerator additive for metal-pretreatment bath processing. The as-supplied material is yellow and odorless, with a pH range of 7.0 to 8.0 and a specific gravity of 1.30 to 1.32. Its liquid form and near-neutral pH provide clear reference points for industrial handling and process control. The grade serves the accelerator-additive role within zinc-phosphating operations, keeping its function focused on controlled metal-pretreatment bath chemistry during production use.

Key features

  • Zinc-Phosphate Accelerator: Serves as a named accelerator additive for zinc-phosphating bath operations.
  • Near-Neutral pH: The as-supplied liquid has a pH range of 7.0 to 8.0.
  • Defined Liquid Profile: The yellow, odorless liquid has a specific gravity of 1.30 to 1.32.
Product Family

BONDERITE M-AD 131

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Yellow Liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.306 - 1.34
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
>121 °C
Chemical Properties
Melting Point
-12

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers