ABLESTIK 539IA

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ABLESTIK 539IA

Main features

  • Polyester-Carrier Epoxy Film
  • 1-Month Work Life at 25 deg C
  • 1-Hour 150 deg C Cure

Product Description

LOCTITE ABLESTIK 539IA is a transparent, non-conductive heat-cure epoxy film adhesive for LCD assembly and bonding difficult metals, plastics, and ceramics. Its polyester carrier provides a uniform bond-line construction, with the film remaining non-conductive after cure. Work life is 1 month at 25 deg C, and heat-cure options are 1 hour at 150 deg C or 2 hours at 125 deg C. Shelf life is 365 days at 0 deg C.

Key features

  • Polyester-carrier construction: Transparent epoxy film uses a polyester carrier with a uniform bond-line format.
  • One-month work life: Work life is 1 month at 25 deg C.
  • Dual heat-cure schedules: Heat cure is 1 hour at 150 deg C or 2 hours at 125 deg C.

Applications

LCD assembly and bonding difficult metals, plastics, and ceramics.

Product Family

ABLESTIK 539IA

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Other Properties
Storage Temperature
-40 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
AppearanceTransparent filmAs supplied
CarrierPolyesterAs supplied
Work life1month25 deg C
Shelf life365days0 deg C