LOCTITE 5607F

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE 5607F

Main features

  • Fluorescent Part B Identification
  • Two-Part Metered Mixing
  • SI 5607 Hardener Component

Product Description

LOCTITE SI 5607F is the fluorescent Part B hardener component used in the LOCTITE SI 5607 two-part silicone system. The component is supplied as a gray paste, with a typical specific gravity of 1.6 to 1.8 at 25 deg C. Typical cone-and-plate viscosity is 20,000 to 35,000 mPa s at 25 deg C and a shear rate of 20 s^-1. Combine this Part B hardener with Part A to form the LOCTITE SI 5607 system. The cured system's bonding, sealing, mechanical, and electrical properties do not apply to LOCTITE SI 5607F alone.

Key features

  • Fluorescent component identification: Fluorescent Part B hardener for the LOCTITE SI 5607 system.
  • Part B viscosity: Typical cone-and-plate viscosity is 20,000 to 35,000 mPa s at 25 deg C and 20 s^-1.
  • Part B specific gravity: Typical specific gravity is 1.6 to 1.8 at 25 deg C for the Part B hardener.
Product Family

LOCTITE 5607F

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray paste
Specific Gravity
1.6 to 1.8
Physical Properties
Viscosity
20,000 to 35,000 mPa.s

Additional Information

Technical properties

As-supplied properties

Values apply to the LOCTITE SI 5607 Part B hardener component only.

PropertyValueUnitMethod / condition
AppearanceGray paste-Part B; as supplied
Specific gravity1.6 to 1.8-Typical; Part B; 25 deg C
Viscosity20,000 to 35,000mPa sTypical; Part B; cone and plate; 25 deg C; shear rate 20 s^-1