ECCOBOND 334-1

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ECCOBOND 334-1

Main features

  • 8-Hour Work Life at 25 deg C
  • Moisture Cure in About 1 to 4 Days
  • One-Part Tungsten-Filled RTV

Product Description

LOCTITE ECCOBOND 334-1 is a one-part, gray tungsten-filled RTV silicone sealant for room-temperature moisture cure. The material is applied without component mixing and has a typical work life of 8 hours at 25 deg C. Cure typically takes about 1 to 4 days at 25 deg C, depending on relative humidity and bond width. Henkel does not recommend bond lines greater than 1 inch wide because moisture cannot readily reach the center of wider sections. After cure, the material forms a relatively flexible silicone seal for applications where a flexible RTV material is specified.

Key features

  • 8-Hour Work Life at 25 deg C: Typical work-life value applies to the one-part RTV silicone before cure.
  • About 1 to 4-Day Moisture Cure: The listed cure range applies at 25 deg C.
  • Tungsten-Filled RTV Silicone: The gray one-part formulation cures to a flexible material without component mixing.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
8 hours

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Work life8h25 deg C; typical
Storage life122days25 deg C; continuously dry; typical
Cure schedule1 to 4days25 deg C; depends on relative humidity and bond width

Leading Brands Trust in Our Products and Services