PERMABOND ET500
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 5 to 8 Minute Handling
- Clear Rapid-Cure Epoxy Bonding
- 12 to 18 MPa Shear
Product Description
PERMABOND ET500 is a clear, two-component epoxy adhesive for rapid structural assembly. Viscosity is 13,000 to 24,000 mPa s, handling time is 5 to 8 minutes at 23 deg C, and shear strength is 12 to 18 MPa. The fast handling profile suits smaller or time-sensitive bonding operations where a clear epoxy is preferred. Applications include bonding wood, metals, ceramics, selected plastics and composites. The resin-and-hardener format provides a structural epoxy bond for multi-material joints while keeping the assembly window short enough for rapid production steps and quick transition from placement to handling.
Key features
- 5 to 8 Minute Handling: Handling time is 5 to 8 minutes at 23 deg C for rapid assembly workflows.
- Clear Two-Part Epoxy: The product is a clear epoxy resin and hardener system for structural bonding.
- 12 to 18 MPa Shear: Shear strength is 12 to 18 MPa.
Applications
Bonding wood, metals, ceramics, selected plastics and composites in small or rapid assembly applications.