MOLYKOTE PG75

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE PG75

Main features

  • Low-Temperature Plastic Lubrication
  • Very Low Friction Performance
  • Long-Term Automotive Mechanism Use

Product Description

MOLYKOTE PG-75 Plastislip Grease is a mineral-oil/polyalphaolefin grease with lithium soap and solid lubricants for plastic/plastic and plastic/metal contacts under light loads. The beige grease has an approximate NLGI 2 consistency, a typical 40 deg C base-oil viscosity of 32 mm^2/s, and a -40 to 130 deg C service range. Its 0.02 coefficient of friction was measured in a steel-ball/POM test at 5 N and 10 cm/s for 24 hours. Applications include vehicle track-rod joints, control cables, gearboxes, planetary gears, sunroof and window mechanisms, and HVAC actuators.

Key features

  • Low-Temperature Contact Lubrication: The typical service range extends to -40 deg C for specified plastic and mixed-material mechanisms.
  • Very Low Friction Performance: The typical coefficient of friction is 0.02 in a steel-ball/POM test at 5 N and 10 cm/s for 24 hours.
  • Long-Term Mechanism Lubrication: Applications include control cables, gear systems, track-rod joints, sunroof mechanisms, and HVAC actuators.

Applications

Automotive and electrical plastic contacts, including track-rod joints, control cables, gearboxes, planetary gears, sunroofs, windows, and HVAC actuators.

Technical Specifications

General Properties
Density (g)
0.86 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorBeige-Typical value
NLGI gradeApprox. 2UnitlessDIN 51818; typical value
Worked penetration270 to 300mm/10ISO 2137; typical value
Density0.86g/mlISO 2811; 20 deg C; typical value
Base-oil viscosity32mm^2/sDIN 51562; 40 deg C; typical value
Dropping point>190deg CISO 2176; typical test result; not a service-temperature limit