MOLYKOTE P-37

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE P-37

Main features

  • Extreme-Heat Fastener Protection
  • High-Load Anti-Seize Performance
  • Low-Seepage Clean Assembly

Product Description

MOLYKOTE P-37 Antiseize Paste is a high-purity mineral-oil and solid-lubricant paste for bolted joints exposed to extreme heat. Its solid-lubricant system has a temperature resistance from -30 to 1,400 deg C, while the typical four-ball weld load is 5,500 N. Low seepage supports use where cleanliness is required, and sulfur content is limited to 250 ppm with total halogen content limited to 200 ppm. The paste is applied to cleaned, fully coated screws, nuts, and bolts made from heat-resistant alloys, including bolted joints used in gas and steam turbines.

Key features

  • Extreme-Heat Threaded Joints: Solid-lubricant temperature resistance ranges from -30 to 1,400 deg C.
  • Four-Ball Weld Load: Typical four-ball weld load is 5,500 N at 1,450 rpm for 1 minute.
  • Controlled Trace Content: Total halogen content is 200 ppm maximum and sulfur content is 250 ppm maximum.

Applications

Screws, nuts, and bolts made from heat-resistant alloys, including high-temperature threaded connections in gas and steam turbines.

Technical Specifications

General Properties
Density (g)
1.21 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceGray black-Typical value
Unworked penetration280 to 310mm/10ISO 2137; typical value
Density1.21g/cm^3ISO 2811; 20 deg C; typical value
Total halogen content200ppmMaximum
Sulfur content250ppmMaximum