MOLYKOTE L-1210
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- ISO VG 100 Compressor Lubrication
- PAO Wide-Temperature Viscosity
- Rust and Oxidation Protection
Product Description
MOLYKOTE L-1210 Synthetic Compressor and Vacuum Pump Oil is an ISO VG 100 PAO synthetic oil for compressor and vacuum-pump lubrication. Its typical kinematic viscosity is 98 cSt at 40 deg C and 14 cSt at 100 deg C, with a viscosity index of 145. The formulation includes rust-and-oxidation additives and has a typical pour point of -48 deg C. Applications include rotary screw vacuum pumps and compressors, with use in other equipment limited to the approved compressor and vacuum-pump applications.
Key features
- ISO VG 100 Profile: Typical viscosity is 98 cSt at 40 deg C for compressor and vacuum-pump lubrication.
- PAO Viscosity and Pour Point: Typical viscosity is 14 cSt at 100 deg C, with a viscosity index of 145 and pour point of -48 deg C.
- Rust and Oxidation Protection: The additive package supports compressor-oil service against rust and oxidation.
Applications
Compressors and vacuum pumps.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical values; not for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| ISO viscosity grade | 100 | - | Manufacturer designation |
| Kinematic viscosity | 98 | cSt | Typical at 40 deg C |
| Kinematic viscosity | 14 | cSt | Typical at 100 deg C |
| Viscosity index | 145 | - | Typical |
| Pour point | -48 | deg C | Typical |
| Specific gravity | 0.841 | - | Typical at 20 deg C |
| Base oil | PAO | - | Typical composition |
| Additive package | R&O | - | Typical composition |