HUMISEAL UV22
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Fast 30-Second UV Handling
- Multi-Substrate Surface Wetting
- Toughened Electronic Bonding
Product Description
HumiSeal UV22 provides a one-part urethane/acrylate adhesive for light-activated electronic and industrial bonding. Its typical viscosity is 20,000 cP, and the material wets and adheres to glass, metals, ceramics, and a range of plastics. Handling condition is reached in 30 seconds using a typical total UV exposure of 1 to 2 J/cm^2. The cured adhesive is clear and toughened, with Shore D75 hardness and a typical operating-temperature range of -20 to 125 deg C. This fast response suits assembly processes that require rapid movement after light exposure.
Key features
- Fast UV handling: Handling condition is reached in 30 seconds with UV exposure.
- Multi-substrate wetting: The adhesive wets and adheres to glass, metals, and a range of plastics.
- Toughened cured adhesive: The cured adhesive is clear and has Shore D75 hardness.
Applications
Electronic and industrial bonding of metals, glass, ceramics, and plastics.
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Values are typical product-selection data and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 20,000 | cP | As supplied; typical |
| Working time | Until UV exposure | As supplied; typical | |
| Handling time | 30 | sec | With UV exposure; typical |
| UV dose | 1 to 2 | J/cm^2 | Total UV exposure; typical |
After-processing / final-state properties
Values describe the UV-cured material and are typical product-selection data, not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Clear | Cured material | |
| Hardness | D75 | Shore D | Cured material; typical |
| Operating temperature | -20 to 125 | deg C | Cured material; typical range |