ELKEM CAF 730 MF
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Neutral system, solvent free and MEKO free
- Non-corrosive
- Low odor
Product Description
ELKEM CAF 730 MF is a one-component, thixotropic silicone elastomer designed for bonding, sealing, protection, and maintenance applications. This neutral-curing, MEKO-free material cures at room temperature upon exposure to atmospheric moisture and is supplied as a non-flowing paste for controlled application. CAF 730 MF is suitable for flexible bonding between metal and plastic components, protection of electronic assemblies, aeronautics sealing applications, and industrial repair and servicing operations. The cured elastomer combines flexibility, dielectric performance, and resistance to thermal aging, making it suitable for applications exposed to demanding environmental and operating conditions.
Key features
- One-component moisture cure: Ready-to-use formulation eliminates mixing and cures at room temperature when exposed to air humidity.
- Flexible silicone elastomer: Typical elongation of 500% and Shore A hardness of approximately 24 support flexible sealing and bonding applications.
- Electrical and thermal performance: Good dielectric properties and continuous operating temperatures from -55°C to +200°C support demanding industrial and electronic applications.
Applications / Suitable for
- Bonding and sealing in aeronautics applications
- Protection of electronic components and assemblies
- Flexible bonding between metal and plastic components
- Industrial maintenance and repair operations
- Transport equipment servicing applications
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Representative as-supplied properties of CAF 730 MF before moisture cure.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Non-flowing paste | — | As supplied |
| Color | White | — | As supplied |
| Specific Gravity | 1.02 | g/cm³ | Typical value |
| Skin Formation Time | 10 | min | 23°C, 50% RH |
| Cured Thickness After 24 h | 4.9 | mm | 23°C, 50% RH |
| Shelf Life | 18 | months | Stored at +2°C to +30°C |
After-processing / final-state properties
Typical properties after moisture cure. Values are provided as guidance and should not be used as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 24 | Shore A | After 7 days cure |
| Tensile Strength | 2.0 | MPa | Approximate, after 7 days cure |
| Elongation | 500 | % | Approximate, after 7 days cure |
| Dielectric Strength | 19 | kV/mm | Approximate |
| Volume Resistivity | 5 × 10¹⁵ | Ω·cm | Approximate |
| Continuous Service Temperature | -55 to +200 | °C | 2 mm film, 1000 h |
| Maximum Peak Temperature | 225 | °C | 2 mm film, 72 h |