DOWSIL SE 9185

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL SE 9185

Main features

  • Fast Tack-Free Room-Temperature Cure
  • High Elongation for Stress Relief
  • Controlled Silicone Volatility

Product Description

DOWSIL SE 9185 is a one-part, non-flowing moisture-cure RTV silicone adhesive/sealant for electronics assembly. The product is described as translucent or white and is designed for sealing PCB system assemblies and modules and for fixing parts on circuit boards. It develops a tack-free surface in 8 minutes at 50% RH and cures at room temperature without mixing or a required oven cure. Typical cured properties include 515% elongation, Shore A 31 hardness, and 435 psi tensile strength, supporting flexible bonds and stress relief. Controlled silicone volatility further supports its use around electronic assemblies.

Key Features

  • One-part moisture-cure RTV
  • Non-flowing formulation
  • 8-minute tack-free time at 50% RH
  • 515% typical cured elongation
  • Controlled silicone volatility
  • Room-temperature cure with optional heat acceleration

Applications / Suitable for

  • Sealing PCB system assemblies and modules
  • Fixing parts on circuit boards

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
515 %
General Properties
Color
The color
Clear or White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05
Physical Properties
Extrusion Rate
246 g/min
Tack-Free Time
6 minutes
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
22 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2.0 E+16 Ohms⋅cm

Additional Information

Electronics assembly silicone adhesive

DOWSIL SE 9185

DOWSIL SE 9185 is a one-part, non-flowing moisture-cure RTV silicone adhesive/sealant developed for electronics assembly. It is used for sealing PCB system assemblies and modules and for fixing parts on circuit boards. The product combines fast tack-free room-temperature cure, high cured elongation for stress relief, and controlled silicone volatility.

One-part RTVNon-flowing8 min tack-free515% elongationControlled volatility

Product profile

Product type
Adhesive / sealant
Components
One part
Chemistry
Polydimethylsiloxane
Cure
Non-corrosive moisture cure at room temperature
Flow behavior
Non-flowing
Color
Translucent or white
Processing and cure

Room-temperature moisture cure with fast surface set

The one-part RTV format eliminates mixing and supports room-temperature processing. Tack-free time is 8 minutes at 50% RH. Cure time for adhesion is 3 to 7 days at 25 deg C. One-part moisture-cure processing is generally performed at room temperature and 30 to 80% relative humidity, with cure progressing from the exposed surface inward. Mild heat below 60 deg C may be used to accelerate cure.

Tack-free time
8 min
At 50% RH
Cure for adhesion
3 to 7 days
At 25 deg C
Heat acceleration
Below 60 deg C
Mild heat may accelerate cure

Dispensing and cure geometry

  • Suitable for automated or manual needle dispensing.
  • Cure proceeds from the exposed surface inward at about 6 mm per 7 days under general one-part moisture-cure guidance.
  • Highly confined spaces or deep-section cure applications are not typically suited to this cure mechanism.

Surface preparation and adhesion

  • Surfaces should be thoroughly cleaned and degreased before bonding.
  • Unprimed adhesion can be achieved on many reactive metals, ceramics and glass, and on selected laminates, resins and plastics.
  • Substrate-specific testing is recommended because surface chemistry, contamination and joint design can materially affect bond performance.
Cured mechanical properties

Flexible cured silicone for stress-relieving bonds

High elongation is a key selection feature of DOWSIL SE 9185. Typical cured properties include 515% elongation, Shore A 31 hardness and 435 psi tensile strength, supporting the product's stated positioning for added stress relief.

Property Typical value Condition / note
Specific gravity 1.05 At 25 deg C
Durometer hardness 29 Shore A Cured material
Tensile strength 435 psi / 3.0 MPa Typical cured value
Elongation 515% Typical cured value

Typical property values are not intended for use as product specifications.

Electrical properties

Electrical insulation data for electronics evaluation

Typical electrical properties include dielectric strength, volume resistivity, dielectric constant and dissipation factor for design evaluation.

Property Typical value Test frequency / note
Dielectric strength 22 kV/mm 550 V/mil
Volume resistivity 2.0 E+16 ohm*cm Typical cured value
Dielectric constant 2.8 At 1 MHz
Dissipation factor 0.0007 At 1 MHz

Typical property values are not intended for use as product specifications. Validate performance in the intended assembly and geometry.

Application fit

Designed for PCB sealing and component fixing

DOWSIL SE 9185 is positioned for boards and assemblies, components and housings where a non-flowing, room-temperature-cure silicone adhesive can provide localized sealing or fixation without two-part mixing.

PCB system assembly sealing

Use for sealing PCB system assemblies and modules. The material is non-flowing and moisture-cures at room temperature.

Circuit-board parts fixing

Use for fixing parts on circuit boards. The product is one-part, non-flowing and designed for room-temperature moisture cure.

Storage and handling

Protect the one-part RTV from premature moisture exposure

Storage

  • Store at or below the storage temperature stated on the product label.
  • Keep the product in its original packaging with the cover tightly attached.
  • Use the material by the Use Before date shown on the product label.

Moisture control

  • Prevent moisture from contacting uncured material during storage.
  • Keep containers tightly closed and minimize headspace.
  • Purge partially filled containers with dry air or another dry gas such as nitrogen.
Product resource

Dow adhesives and sealants selection guide

Review DOWSIL SE 9185 alongside other Dow electronics adhesives and sealants, including cure system, processing behavior and comparative typical properties.

View the Dow adhesives and sealants selection guide
Technical support

Evaluate DOWSIL SE 9185 for your electronics assembly

Discuss PCB sealing, component fixing, joint geometry, dispensing, cure conditions and substrate compatibility with the technical team.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers