DOWSIL 8257

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 8257

Main features

  • 1:1 Silicone Foam Mixing
  • 25 Shore 00 Cured Hardness
  • Integrated Compression Gasket Formation

Product Description

SILASTIC 8257 Silicone Foam is a two-part silicone foam system mixed 1:1 and cured directly on parts at room temperature to form an integrated compression gasket. Typical cured hardness is 25 Shore 00. Post-cured material has low compression set retained at high service temperatures and remains stable and flexible across a wide temperature range. Applications include automotive parts, electrical-device housings, exterior lighting, domestic-appliance components, and tile-printing rollers.

Key features

  • Equal-ratio foam mixing: The two components mix at a 1:1 ratio.
  • Cured foam hardness: Typical cured hardness is 25 Shore 00.
  • Integrated compression gasket formation: The foam is dispensed and cured directly on parts to form a compression gasket.

Applications

Automotive parts; electrical-device housings; exterior lighting; domestic-appliance components; tile-printing rollers.

Product Family

DOWSIL 8257

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part (A/B)
Density (g)
1.1 - 1.6 g/cm3
Physical Properties
Tack-Free Time
maximum 10 minutes