CONATHANE EN-21

Main features

  • Low-viscosity
  • Room-temperature cure
  • Good electrical and thermal properties

Product Description

CONATHANE® EN-21 Polyurethane Encapsulant is a two-component, unfilled, low-viscosity polyurethane potting compound for electronic circuits, components, and power devices. The system supports hand-mix, meter-mix, and vacuum potting or casting processes and may cure at room temperature or with low-temperature heat. Documented applications include transformers, coils, reed and mercury switches, inductors, ignition systems, voltage regulators, ballasts, microcircuits, rectifiers, and printed circuit assemblies. Typical cured properties include Shore A 80 hardness, 155% elongation, 0.3 W/m·K thermal conductivity, moisture resistance, and thermal-shock performance.

Key features

  • Low-viscosity processing: Typical initial mixed viscosity is 2,000 cP at 25°C.
  • Room-temperature or heat cure: Recommended cure options are seven days at 25°C or four hours at 80°C.
  • Electrical and thermal properties: Typical data include 650 V/mil dielectric strength and 0.3 W/m·K thermal conductivity.

Applications / Suitable for

  • Transformers, coils, switches, and inductors
  • Voltage regulators, ballasts, and rectifiers
  • Microcircuits and printed circuit assemblies

Technical Specifications

General Properties
Color
Clear Amber / Clear Amber
Component System
Two (Urethane Prepolymer / Curative)
Specific Gravity
1.14 / 0.96
Electrical Properties
Dielectric Strength
25.6 kV/mm
Volume Resistivity
7.2 x 10¹⁴ Ohms⋅cm
Chemical Properties
Water Absorption
0.07 %
Thermal Properties
Thermal Conductivity
0.3 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A viscosity 6,000 cP At 25°C
Part B viscosity 800 cP At 25°C
Part A specific gravity 1.14 N/A At 25°C
Part B specific gravity 0.96 N/A At 25°C
Mix ratio 100:116 parts by weight Part A : Part B
Initial mixed viscosity 2,000 cP At 25°C
Pot life 40 min At 25°C
Cure options 7 days at 25°C; 4 h at 80°C N/A Recommended schedules
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 80 Shore A ASTM D2240 at 25°C
Tensile strength 2,000 psi ASTM D412 at 25°C
Ultimate elongation 155 % ASTM D412 at 25°C
Tear strength 120 pli ASTM D624 at 25°C
Dielectric strength 650 V/mil ASTM D149, 1/16 in specimen
Volume resistivity 7.2 × 10¹⁴ ohm·cm ASTM D257 at 25°C
Thermal conductivity 0.3 W/m·K ASTM C177 at 25°C
Coefficient of thermal expansion 210 ppm/°C ASTM D696 at 25°C