BOSTIK FPA110-1FR

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK FPA110-1FR

Main features

  • Heat-Activated Decorative Lamination
  • Platen or Vacuum-Bag Processing
  • Removable for Interior Refurbishment

Product Description

Bostik FPA110-1FR is a flame-retardant thermoplastic adhesive film for transportation and aerospace decorative laminates. The 1 mil film bonds materials including PVF, vinyl, aluminum, polyamide film, phenolic prepreg, fabrics, and wools. It is heat activated at 220 to 235 deg F and can be processed by platen press or vacuum bag methods, with vacuum-bag pressure guidance of 20 to 50 psi. The adhesive is removable during refurbishment and has a SAFT heat resistance of 200 deg F, making it suited to decorative interior constructions where controlled heat activation and later removal are important.

Key features

  • Heat-activated bonding: Activation at 220 to 235 deg F provides a defined thermal bonding window.
  • Platen or vacuum-bag processing: Can be bonded by platen press or vacuum bag methods.
  • Refurbishment removal: The thermoplastic adhesive can be removed during interior refurbishment.

Applications

Transportation and aerospace decorative-laminate bonding to PVF, vinyl, aluminum, polyamide, phenolic prepreg, fabrics, and wools.

Product Family

BOSTIK FPA110-1FR

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Off-white
Density (g)
1.6 g/cm3
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
25 µm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceOff-whiteAs supplied
Film weight32g/m^2As supplied
Density1.6g/cm^325 deg C
Film thickness1.0milTDS also gives 25 um
Shelf life24monthsStored dry at 40 to 80 deg F