ARADUR HY 1102
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Liquid Anhydride Curing Agent
- Unmodified Anhydride Chemistry
- Filament Winding and RTM Use
Product Description
ARADUR HY 1102 is a liquid, unmodified anhydride curing agent for epoxy systems used in filament winding, impregnation, pultrusion, and resin-transfer molding. It serves as the curing-agent component in composite processing and in electrical insulating and impregnating systems. HY 1102 is used with an epoxy resin rather than applied as a standalone adhesive.
Key features
- Anhydride curing chemistry: HY 1102 is supplied as a liquid, unmodified anhydride curing agent.
- Composite processing routes: Applications include filament winding, pultrusion, and resin-transfer molding.
- Electrical impregnation role: The curing agent is used as a component in electrical insulating and impregnating systems.
Applications
Filament winding, impregnation, pultrusion, resin-transfer molding, and electrical insulating or impregnating epoxy systems.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
Viscosity
50 - 70 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application
General Properties
Appearance
Clear liquid
Appearance at room temperature.
Density (g)
1.13 – 1.17 g/cm3
Thermal Properties
Flash Point
145 °C
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor.
Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.